Final Magnetic Moment2.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.764 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.189 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGa4Bi2O9 + Fe2O3 + Bi2O3 |
Band Gap1.741 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbam [55] |
Hall-P 2 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 285.1 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 286.5 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 331.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 244.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 132.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 66.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 331.1 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 149.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 132.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 165.7 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 248.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 142.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 66.2 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 331.1 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 199.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 66.2 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 331.1 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 248.5 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 348.4 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 264.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 331.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 286.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 190.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 331.1 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 331.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 199.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 198.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 237.6 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 248.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 348.4 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 264.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 199.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 163.0 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 298.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 264.9 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 248.5 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 68.8 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 49.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 237.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 237.6 |
BN (mp-984) | <1 1 1> | <0 0 1> | 237.6 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 1> | 286.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 248.8 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 1 0> | 248.5 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 132.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 298.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 82.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 348.4 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 199.1 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 95.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Eu2Al4O9 (mp-771815) | 0.4387 | 0.101 | 3 |
La2Ga4O9 (mp-771697) | 0.4138 | 0.088 | 3 |
Ga4Bi2O9 (mp-23519) | 0.1503 | 0.000 | 3 |
Fe4Bi2O9 (mp-540741) | 0.2064 | 0.012 | 3 |
Al4Bi2O9 (mvc-16101) | 0.2347 | 0.000 | 3 |
LiFe2O2F3 (mp-780549) | 0.5433 | 0.064 | 4 |
Li2Co4O3F8 (mp-780832) | 0.5506 | 0.263 | 4 |
Li2Fe4O3F8 (mp-780815) | 0.5945 | 0.523 | 4 |
Li2V4O3F8 (mp-766905) | 0.6000 | 0.065 | 4 |
Li2Mn4O3F8 (mp-765991) | 0.5712 | 0.571 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Ga_d Fe_pv Bi O |
Final Energy/Atom-5.9979 eV |
Corrected Energy-201.3285 eV
Uncorrected energy = -179.9385 eV
Composition-based energy adjustment (-0.687 eV/atom x 18.0 atoms) = -12.3660 eV
Composition-based energy adjustment (-2.256 eV/atom x 4.0 atoms) = -9.0240 eV
Corrected energy = -201.3285 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)