Final Magnetic Moment0.006 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.419 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.051 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi5P4 + SiNi + NiP2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 204.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 204.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 204.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 204.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 233.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 292.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 321.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 292.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 204.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 321.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 87.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 292.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 204.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 321.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 262.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 262.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 321.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 233.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 321.1 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 204.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 350.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 204.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 146.0 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 204.4 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 204.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 292.0 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 292.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 204.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 146.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 262.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 87.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 262.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 204.4 |
BN (mp-984) | <1 1 1> | <0 0 1> | 204.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 292.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 233.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 321.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 233.6 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 262.8 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 321.1 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 233.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 146.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 175.2 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 233.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 321.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 204.4 |
C (mp-66) | <1 1 0> | <0 0 1> | 87.6 |
C (mp-66) | <1 1 1> | <0 0 1> | 87.6 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 233.6 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 146.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni5Ge2P3 (mp-662818) | 0.2599 | 0.043 | 3 |
Si4MoPt3 (mp-978785) | 0.4949 | 0.000 | 3 |
SiNi2As (mp-21598) | 0.3471 | 0.040 | 3 |
Ni2GeP (mp-618929) | 0.2937 | 0.022 | 3 |
SiNi2P (mp-510422) | 0.4351 | 0.022 | 3 |
TiTlCuTe3 (mp-9344) | 0.6382 | 0.000 | 4 |
RbHfAgTe3 (mp-9780) | 0.6768 | 0.000 | 4 |
ZrSb2 (mp-979) | 0.5536 | 0.000 | 2 |
HfSb2 (mp-2180) | 0.5329 | 0.000 | 2 |
ZrBi2 (mp-29642) | 0.5384 | 0.000 | 2 |
Mg4Si3 (mp-1078478) | 0.5349 | 0.260 | 2 |
CrBi (mp-1079128) | 0.5369 | 0.609 | 2 |
Bi (mp-1067758) | 0.7266 | 0.086 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si Ni_pv P |
Final Energy/Atom-6.0184 eV |
Corrected Energy-481.4736 eV
-481.4736 eV = -481.4736 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)