Final Magnetic Moment1.980 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.542 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.266 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 159.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 163.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 159.1 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 159.1 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 159.1 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 159.1 |
C (mp-48) | <1 0 1> | <0 0 1> | 159.1 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 159.1 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 -1> | 164.9 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 159.1 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 163.3 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 159.1 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 159.1 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 159.1 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 159.1 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 159.1 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 159.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaSi2O5 (mp-29755) | 0.7108 | 0.093 | 3 |
V3P4Pb2O17 (mp-683863) | 0.7408 | 0.096 | 4 |
KVCdO4 (mp-578796) | 0.7147 | 0.000 | 4 |
Al2P2O11F (mp-653569) | 0.7358 | 0.507 | 4 |
BaV2(PO5)2 (mp-19512) | 0.7091 | 0.000 | 4 |
Sb4S3N6(OF)12 (mp-1006611) | 0.6847 | 0.896 | 5 |
KAl2P2H8O12F (mp-698033) | 0.7371 | 0.007 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: K_sv Fe_pv P O |
Final Energy/Atom-6.6430 eV |
Corrected Energy-582.4657 eV
Uncorrected energy = -531.4417 eV
Composition-based energy adjustment (-0.687 eV/atom x 48.0 atoms) = -32.9760 eV
Composition-based energy adjustment (-2.256 eV/atom x 8.0 atoms) = -18.0480 eV
Corrected energy = -582.4657 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)