Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.629 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.058 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPNCl2 + C6N7Cl3 + P4N3Cl11 |
Band Gap3.497 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 1 0> | <0 0 1> | 117.8 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 163.8 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 163.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 235.7 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 235.7 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 117.8 |
Ni (mp-23) | <1 0 0> | <1 0 -1> | 184.8 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 163.8 |
MoSe2 (mp-1634) | <1 1 1> | <0 1 0> | 176.2 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 -1> | 184.8 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 163.8 |
Cu (mp-30) | <1 1 0> | <1 0 -1> | 184.8 |
TiO2 (mp-390) | <1 0 1> | <0 0 1> | 117.8 |
Fe2O3 (mp-24972) | <0 0 1> | <1 0 -1> | 184.8 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 163.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HCO (mp-995234) | 0.7019 | 0.265 | 3 |
Be(N3O7)2 (mp-30141) | 0.6375 | 0.056 | 3 |
PHN2 (mp-35220) | 0.6931 | 0.002 | 3 |
P6N7Cl9 (mp-650015) | 0.5674 | 0.002 | 3 |
S5N4O3 (mp-540558) | 0.6401 | 0.199 | 3 |
P3CN4Cl7 (mp-638206) | 0.2580 | 0.022 | 4 |
P3H4N5Cl4 (mp-705530) | 0.5822 | 0.037 | 4 |
PCN2Cl3 (mp-679969) | 0.6078 | 0.044 | 4 |
P3H11N4O9 (mp-695955) | 0.6127 | 0.084 | 4 |
BS4N4F3 (mp-16813) | 0.5962 | 0.111 | 4 |
SiO2 (mp-673168) | 0.6231 | 0.681 | 2 |
ZnH8C4(NO3)2 (mp-655017) | 0.6266 | 0.584 | 5 |
LiAlSiH2O5 (mp-604420) | 0.5513 | 0.105 | 5 |
PH6CNO3 (mp-554756) | 0.5898 | 0.049 | 5 |
ZnH8C4(NO3)2 (mp-601243) | 0.6235 | 0.584 | 5 |
P5H5N6(Cl4O)2 (mp-707469) | 0.5145 | 0.021 | 5 |
AlSi2HC6NCl3 (mp-710380) | 0.5226 | 0.885 | 6 |
B2H10C2NClO3 (mp-554977) | 0.7028 | 0.158 | 6 |
PH8C2SNO2 (mp-561476) | 0.7465 | 0.119 | 6 |
B2H10C2NClO3 (mp-554598) | 0.6264 | 0.156 | 6 |
Al2P3H17C4(NO6)2 (mp-709723) | 0.6987 | 0.057 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: P C N Cl |
Final Energy/Atom-5.5298 eV |
Corrected Energy-464.5060 eV
-464.5060 eV = -464.5060 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)