Final Magnetic Moment1.465 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.623 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.014 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.42 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaCuF3 + NaFeF4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 294.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 196.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 196.5 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 196.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 196.5 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 196.5 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 157.3 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 196.5 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 221.3 |
BN (mp-984) | <0 0 1> | <1 0 0> | 98.2 |
BN (mp-984) | <1 1 0> | <1 0 0> | 98.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 196.5 |
CdTe (mp-406) | <1 0 0> | <1 0 -1> | 221.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 282.0 |
Al (mp-134) | <1 1 1> | <1 0 0> | 196.5 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 183.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 282.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 94.0 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 282.0 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 282.0 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 154.6 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 282.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 0 0> | 196.5 |
C (mp-66) | <1 1 1> | <1 0 0> | 196.5 |
LaF3 (mp-905) | <1 0 0> | <1 0 -1> | 110.6 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 94.0 |
PbS (mp-21276) | <1 1 1> | <1 0 0> | 196.5 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 294.7 |
InSb (mp-20012) | <1 0 0> | <1 0 -1> | 221.3 |
PbSe (mp-2201) | <1 1 1> | <1 0 0> | 196.5 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 188.0 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 282.0 |
Si (mp-149) | <1 0 0> | <1 0 0> | 294.7 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 -1> | 110.6 |
CdSe (mp-2691) | <1 1 1> | <1 0 0> | 196.5 |
C (mp-48) | <0 0 1> | <1 0 0> | 294.7 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 196.5 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 1> | 157.3 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 282.0 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 1> | 157.3 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 -1> | 110.6 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 -1> | 221.3 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 294.7 |
TiO2 (mp-390) | <1 0 1> | <1 0 1> | 157.3 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 188.0 |
ZnO (mp-2133) | <0 0 1> | <1 0 0> | 196.5 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 282.0 |
GaSb (mp-1156) | <1 1 1> | <1 0 0> | 196.5 |
Cu (mp-30) | <1 0 0> | <1 0 -1> | 221.3 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 -1> | 110.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2Ta2O7 (mp-640836) | 0.4326 | 0.000 | 3 |
Na2Te2O7 (mp-20254) | 0.4871 | 0.000 | 3 |
Mn2Sb2O7 (mp-562121) | 0.4482 | 0.017 | 3 |
Sr2Sb2O7 (mp-4103) | 0.5079 | 0.000 | 3 |
Ag2Te2O7 (mp-13211) | 0.4981 | 0.002 | 3 |
Na2FeCuF7 (mp-578795) | 0.2877 | 0.014 | 4 |
Na2ZnFeF7 (mp-560220) | 0.3340 | 0.177 | 4 |
Na2GaCuF7 (mp-21552) | 0.2355 | 0.020 | 4 |
Na2ZnFeF7 (mp-700268) | 0.3370 | 0.177 | 4 |
Na2FeCuF7 (mp-654249) | 0.3545 | 0.014 | 4 |
Pb3O5 (mp-651870) | 0.6352 | 0.042 | 2 |
Ca5Gd3Ti5Mn3O24 (mp-744410) | 0.7168 | 0.013 | 5 |
SrLiEuTeO6 (mp-676932) | 0.6623 | 0.056 | 5 |
LiCaPrTeO6 (mp-40186) | 0.6881 | 0.024 | 5 |
Na3Ca2Ta3Ti2O15 (mp-677743) | 0.7041 | 0.011 | 5 |
LaMgCrNiO6 (mvc-9871) | 0.7099 | 0.423 | 5 |
NaYTiNbO6F (mp-42599) | 0.6512 | 0.053 | 6 |
NaGdTiNbO6F (mp-42981) | 0.6829 | 0.047 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Na_pv Fe_pv Cu_pv F |
Final Energy/Atom-4.4234 eV |
Corrected Energy-216.5875 eV
Uncorrected energy = -194.6275 eV
Composition-based energy adjustment (-0.462 eV/atom x 28.0 atoms) = -12.9360 eV
Composition-based energy adjustment (-2.256 eV/atom x 4.0 atoms) = -9.0240 eV
Corrected energy = -216.5875 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)