Final Magnetic Moment0.021 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.857 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.29 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.667 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP41212 [92] |
HallP 4abw 2nw |
Point Group422 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 285.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 285.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 190.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 285.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 285.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 285.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 285.0 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 285.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 285.0 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 285.0 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 180.6 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 285.0 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 190.0 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 190.0 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 153.6 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 285.0 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 285.0 |
C (mp-48) | <1 0 0> | <1 0 0> | 153.6 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 95.0 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 190.0 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 190.0 |
TiO2 (mp-390) | <1 1 0> | <1 0 0> | 153.6 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 190.0 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 285.0 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 190.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cs2Si2Se5 (mp-542550) | 0.3835 | 0.000 | 3 |
Tl2Ge2Se5 (mp-540818) | 0.3706 | 0.000 | 3 |
K2Ge2S5 (mp-541878) | 0.2827 | 0.000 | 3 |
Rb2Ge2S5 (mp-541879) | 0.3208 | 0.000 | 3 |
Rb2Ge2Se5 (mp-541880) | 0.3080 | 0.000 | 3 |
AgH2ClO5 (mp-24053) | 0.6595 | 0.002 | 4 |
Cs2AgAsS4 (mp-561622) | 0.6567 | 0.000 | 4 |
K2Cu(PS3)3 (mp-559644) | 0.4277 | 0.000 | 4 |
KCuP2Se5 (mp-622199) | 0.6279 | 0.000 | 4 |
Cs2AgSbS4 (mp-510710) | 0.6079 | 0.000 | 4 |
FeCl3 (mp-676241) | 0.6850 | 0.024 | 2 |
P2S7 (mp-1006118) | 0.6802 | 0.003 | 2 |
RbCdH2I3O (mp-634062) | 0.7133 | 0.003 | 5 |
Na6Zn3As4H6O19 (mp-758925) | 0.6882 | 0.003 | 5 |
Na6Zn3P4H6O19 (mp-24507) | 0.7086 | 0.008 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: B Pb_d S |
Final Energy/Atom-5.0959 eV |
Corrected Energy-387.0280 eV
Uncorrected energy = -366.9080 eV
Composition-based energy adjustment (-0.503 eV/atom x 40.0 atoms) = -20.1200 eV
Corrected energy = -387.0280 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)