Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.154 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.039 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCd(NO3)2 + CsNO3 + CdO + N2 |
Band Gap2.408 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 217.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 163.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 271.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 217.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 54.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 228.6 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 54.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 152.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 217.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 264.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 187.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 163.0 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 280.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 217.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 163.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 217.3 |
BN (mp-984) | <1 1 0> | <1 0 0> | 304.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 163.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 217.3 |
Al (mp-134) | <1 1 0> | <1 0 0> | 228.6 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 217.3 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 280.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 217.3 |
TiO2 (mp-2657) | <0 0 1> | <1 0 1> | 280.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 152.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 163.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 217.3 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 264.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 217.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 228.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 325.9 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 217.3 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 1> | 187.2 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 152.4 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 264.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 228.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 54.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 163.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 228.6 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 228.6 |
LaF3 (mp-905) | <1 0 0> | <1 0 1> | 280.7 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 304.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 217.3 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 280.7 |
PbS (mp-21276) | <1 0 0> | <1 0 1> | 280.7 |
GaP (mp-2490) | <1 0 0> | <1 0 1> | 93.6 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 132.0 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 54.3 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 280.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 217.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
44 | 20 | 23 | 1 | -1 | 0 |
20 | 44 | 23 | -1 | 1 | 0 |
23 | 23 | 47 | 0 | 0 | 0 |
1 | -1 | 0 | 16 | 0 | 1 |
-1 | 1 | 0 | 0 | 16 | 1 |
0 | 0 | 0 | 1 | 1 | 12 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
33.1 | -8.7 | -12.1 | -3.1 | 2.9 | -0.0 |
-8.7 | 33.1 | -12.1 | 3.1 | -2.9 | 0.0 |
-12.1 | -12.1 | 33.2 | -0.0 | 0.0 | -0.0 |
-3.1 | 3.1 | -0.0 | 64.8 | 0.0 | -5.7 |
2.9 | -2.9 | 0.0 | -0.0 | 64.8 | -6.1 |
-0.0 | 0.0 | 0.0 | -5.7 | -6.1 | 83.5 |
Shear Modulus GV13 GPa |
Bulk Modulus KV30 GPa |
Shear Modulus GR13 GPa |
Bulk Modulus KR30 GPa |
Shear Modulus GVRH13 GPa |
Bulk Modulus KVRH30 GPa |
Elastic Anisotropy0.17 |
Poisson's Ratio0.31 |
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.10176 | -0.10176 | 0.00000 | -0.02004 | -0.00144 | 0.03422 |
0.03422 | -0.03422 | 0.00000 | -0.00143 | 0.02004 | -0.10176 |
-0.06735 | -0.06735 | -0.05130 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.15316 C/m2 |
Crystallographic Direction vmax |
---|
-3.00000 |
1.00000 |
-0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.98 | 0.00 | 0.00 |
-0.00 | 2.98 | 0.00 |
-0.00 | 0.00 | 2.96 |
Dielectric Tensor εij (total) |
||
---|---|---|
8.06 | 0.00 | 0.00 |
-0.00 | 8.06 | 0.00 |
-0.00 | 0.00 | 6.50 |
Polycrystalline dielectric constant
εpoly∞
2.98
|
Polycrystalline dielectric constant
εpoly
7.54
|
Refractive Index n1.73 |
Potentially ferroelectric?Unknown |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Cd N O |
Final Energy/Atom-5.8021 eV |
Corrected Energy-67.9447 eV
Uncorrected energy = -63.8227 eV
Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV
Corrected energy = -67.9447 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)