Final Magnetic Moment-0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.943 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.217 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToOsS2 + Os + CO2 + C |
Band Gap1.713 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <1 0 -1> | 179.7 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 122.5 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 122.5 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 122.5 |
SiC (mp-11714) | <1 1 0> | <0 1 -1> | 163.7 |
SiC (mp-11714) | <1 1 1> | <1 -1 0> | 167.9 |
C (mp-48) | <0 0 1> | <0 1 -1> | 163.7 |
C (mp-48) | <1 0 1> | <1 0 -1> | 179.7 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 122.5 |
LiAlO2 (mp-3427) | <1 0 1> | <1 -1 0> | 167.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Os6C17S2O17 (mp-648264) | 0.5247 | 0.194 | 4 |
Fe6Sn2(CO)23 (mp-653267) | 0.4833 | 0.620 | 4 |
Ru6C17S2O17 (mp-650984) | 0.5053 | 0.418 | 4 |
Ru7C20(SO10)2 (mp-650996) | 0.4760 | 0.200 | 4 |
H2Ru6(CO)17 (mp-720808) | 0.4734 | 0.236 | 4 |
Os6C19O20 (mp-648157) | 0.6931 | 0.223 | 3 |
Os5(CO)19 (mp-680286) | 0.7256 | 0.229 | 3 |
Os(CO)4 (mp-679947) | 0.6675 | 0.229 | 3 |
Ir3(CO)8 (mp-667400) | 0.7326 | 0.221 | 3 |
HOs3C10ClO10 (mp-706652) | 0.6298 | 0.180 | 5 |
H2Ru6C18SO20 (mp-720807) | 0.6842 | 0.186 | 5 |
HOs6C18S2O19 (mp-707923) | 0.5154 | 0.207 | 5 |
H2Os4Pt(CO)15 (mp-740758) | 0.6107 | 0.227 | 5 |
CoHRu3(CO)13 (mp-735485) | 0.6069 | 0.266 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points4 |
U Values-- |
PseudopotentialsVASP PAW: Os_pv C S O |
Final Energy/Atom-8.1983 eV |
Corrected Energy-765.8587 eV
-765.8587 eV = -737.8447 eV (uncorrected energy) - 28.0139 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)