Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.109 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.022 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAlPO4 |
Band Gap5.428 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmc21 [36] |
HallC 2c 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
InAs (mp-20305) | <1 1 1> | <0 1 0> | 128.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 256.5 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 256.5 |
Al (mp-134) | <1 1 1> | <0 1 0> | 256.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 128.2 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 256.5 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 256.5 |
PbS (mp-21276) | <1 1 1> | <0 1 0> | 128.2 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 256.5 |
InP (mp-20351) | <1 1 1> | <0 1 0> | 128.2 |
Ni (mp-23) | <1 1 1> | <0 1 0> | 128.2 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 256.5 |
CdSe (mp-2691) | <1 1 1> | <0 1 0> | 128.2 |
WSe2 (mp-1821) | <1 0 0> | <0 1 0> | 256.5 |
WSe2 (mp-1821) | <1 1 0> | <0 1 0> | 256.5 |
WSe2 (mp-1821) | <1 1 1> | <0 1 0> | 256.5 |
GaSb (mp-1156) | <1 1 1> | <0 1 0> | 128.2 |
Al2O3 (mp-1143) | <0 0 1> | <0 1 0> | 256.5 |
ZnTe (mp-2176) | <1 1 1> | <0 1 0> | 128.2 |
CaCO3 (mp-3953) | <1 0 0> | <0 1 0> | 256.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VBO4 (mp-771386) | 0.5153 | 0.068 | 3 |
AlPO4 (mp-558088) | 0.3177 | 0.025 | 3 |
AlPO4 (mp-683883) | 0.5402 | 0.018 | 3 |
AlPO4 (mp-560815) | 0.5246 | 0.030 | 3 |
CoPO4 (mp-694829) | 0.5484 | 0.196 | 3 |
RbAlSiO4 (mp-6434) | 0.7133 | 0.000 | 4 |
CsSi3HO7 (mp-758180) | 0.4110 | 0.002 | 4 |
CsSi2HO5 (mp-557780) | 0.5903 | 0.005 | 4 |
RbP(HO2)2 (mp-703528) | 0.6486 | 0.007 | 4 |
KAlSi3O8 (mp-697670) | 0.7266 | 0.000 | 4 |
SiO2 (mp-680222) | 0.4550 | 0.032 | 2 |
SiO2 (mp-558569) | 0.4842 | 0.073 | 2 |
SiO2 (mp-646895) | 0.4700 | 0.014 | 2 |
CeSe2 (mp-1080632) | 0.4682 | 0.522 | 2 |
SiO2 (mp-644923) | 0.4800 | 0.011 | 2 |
RbB2P2HO9 (mp-758281) | 0.6893 | 0.000 | 5 |
Explore more synthesis descriptions for materials of composition AlPO4.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Al P O |
Final Energy/Atom-7.4658 eV |
Corrected Energy-855.7710 eV
Uncorrected energy = -806.3070 eV
Composition-based energy adjustment (-0.687 eV/atom x 72.0 atoms) = -49.4640 eV
Corrected energy = -855.7710 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)