Final Magnetic Moment0.167 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.040 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.238 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap0.957 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4 [82] |
HallI 4 |
Point Group4 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5440) | 0.6645 | 0.012 | 3 |
AlPO4 (mp-558056) | 0.6675 | 0.011 | 3 |
Si2H2O5 (mp-626037) | 0.6568 | 0.035 | 3 |
AlPO4 (mp-667363) | 0.6724 | 0.014 | 3 |
AlPO4 (mp-1019510) | 0.6339 | 0.010 | 3 |
RbAlSiO4 (mp-6434) | 0.7198 | 0.000 | 4 |
CsSi3HO7 (mp-758180) | 0.7373 | 0.002 | 4 |
Cs2MgSi5O12 (mp-1019610) | 0.7125 | 0.000 | 4 |
Rb2CdSi5O12 (mp-15125) | 0.7159 | 0.000 | 4 |
Rb2MgSi5O12 (mp-1020860) | 0.6932 | 0.000 | 4 |
SiO2 (mp-600080) | 0.5450 | 0.022 | 2 |
SiO2 (mp-600054) | 0.5539 | 0.018 | 2 |
SiO2 (mp-34150) | 0.5306 | 0.341 | 2 |
SiO2 (mp-639558) | 0.5493 | 0.015 | 2 |
SiO2 (mp-600065) | 0.5303 | 0.021 | 2 |
K6Al11Si13Ag5O48 (mp-686585) | 0.7497 | 0.171 | 5 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.6783 eV |
Corrected Energy-1173.0969 eV
-1173.0969 eV = -1105.6771 eV (uncorrected energy) - 67.4198 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)