Final Magnetic Moment11.291 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.196 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.092 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnSiNi + Mn6Si7Ni16 + Mn |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 161.2 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 114.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 197.4 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 161.2 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 197.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 197.4 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 161.2 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 161.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 227.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 197.4 |
Al (mp-134) | <1 1 1> | <1 1 1> | 197.4 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 227.9 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 161.2 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 114.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 161.2 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 1 1> | 197.4 |
C (mp-66) | <1 0 0> | <1 0 0> | 114.0 |
C (mp-66) | <1 1 0> | <1 1 0> | 161.2 |
C (mp-66) | <1 1 1> | <1 1 1> | 197.4 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 227.9 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 227.9 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 114.0 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 161.2 |
PbSe (mp-2201) | <1 1 1> | <1 1 1> | 197.4 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 227.9 |
Au (mp-81) | <1 0 0> | <1 0 0> | 227.9 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 161.2 |
CdSe (mp-2691) | <1 1 1> | <1 1 1> | 197.4 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 114.0 |
CaCO3 (mp-3953) | <0 0 1> | <1 1 1> | 197.4 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 114.0 |
YAlO3 (mp-3792) | <1 0 0> | <1 1 0> | 161.2 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 114.0 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 161.2 |
TiO2 (mp-390) | <1 0 1> | <1 1 0> | 161.2 |
ZnO (mp-2133) | <0 0 1> | <1 1 1> | 197.4 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 161.2 |
GaSb (mp-1156) | <1 1 1> | <1 1 1> | 197.4 |
GaTe (mp-542812) | <1 0 0> | <1 0 0> | 227.9 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 161.2 |
ZnTe (mp-2176) | <1 1 1> | <1 1 1> | 197.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn3SiNi2 (mp-17260) | 0.1130 | 0.000 | 3 |
V3SiNi2 (mp-504625) | 0.3137 | 0.107 | 3 |
Al2Re3B (mp-18503) | 0.0576 | 0.578 | 3 |
Nb3Co2Si (mp-505627) | 0.4479 | 0.040 | 3 |
Zn3Ni2Ge (mp-16227) | 0.2119 | 0.002 | 3 |
Ti2Ni (mp-1808) | 0.2035 | 0.000 | 2 |
Sc2Ni (mp-867501) | 0.1415 | 0.000 | 2 |
Hf2Fe (mp-2754) | 0.2187 | 0.000 | 2 |
Nb5Ni (mp-669699) | 0.2147 | 0.207 | 2 |
Zr2Cu (mp-583800) | 0.2613 | 0.068 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mn_pv Si Ni_pv |
Final Energy/Atom-7.6073 eV |
Corrected Energy-182.5750 eV
Uncorrected energy = -182.5750 eV
Corrected energy = -182.5750 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)