Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-2.804 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.647 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPna21 [33] |
HallP 2c 2n |
Point Groupmm2 |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 140.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 211.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 211.0 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 164.7 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 172.4 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 164.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 211.0 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 164.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 281.3 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 86.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 70.3 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 86.2 |
TeO2 (mp-2125) | <1 0 1> | <0 1 1> | 222.5 |
LiTaO3 (mp-3666) | <1 1 1> | <0 1 0> | 258.7 |
MgO (mp-1265) | <1 0 0> | <1 1 0> | 164.7 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 281.3 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 86.2 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 172.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 0 1> | 157.0 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 0> | 140.3 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 0> | 140.3 |
PbS (mp-21276) | <1 1 0> | <1 0 1> | 157.0 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 211.0 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 172.4 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 211.0 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 157.0 |
InSb (mp-20012) | <1 0 0> | <0 1 0> | 86.2 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 211.0 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 211.0 |
SiC (mp-11714) | <1 0 1> | <0 1 1> | 222.5 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 211.0 |
MoSe2 (mp-1634) | <1 0 1> | <0 0 1> | 211.0 |
Si (mp-149) | <1 0 0> | <0 0 1> | 211.0 |
C (mp-48) | <0 0 1> | <0 0 1> | 211.0 |
NaCl (mp-22862) | <1 0 0> | <1 1 0> | 164.7 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 1> | 157.0 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 172.4 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 164.7 |
TiO2 (mp-390) | <1 0 1> | <0 0 1> | 281.3 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 211.0 |
TiO2 (mp-390) | <1 1 1> | <0 0 1> | 211.0 |
MgF2 (mp-1249) | <0 0 1> | <0 1 0> | 86.2 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 140.6 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 70.3 |
Cu (mp-30) | <1 0 0> | <1 0 1> | 157.0 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 281.3 |
Ge (mp-32) | <1 0 0> | <1 1 0> | 164.7 |
Al2O3 (mp-1143) | <1 0 0> | <0 1 0> | 258.7 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 211.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsTiAsO5 (mp-541956) | 0.3153 | 0.000 | 4 |
RbTiAsO5 (mp-6394) | 0.2835 | 0.000 | 4 |
KVPO5 (mp-19517) | 0.2761 | 0.000 | 4 |
KTiPO5 (mp-6268) | 0.2469 | 0.000 | 4 |
RbTiPO5 (mp-6539) | 0.1299 | 0.000 | 4 |
MoO2 (mvc-6944) | 0.5324 | 0.290 | 2 |
VO2 (mvc-6918) | 0.5891 | 0.100 | 2 |
CrO2 (mvc-11581) | 0.6116 | 0.166 | 2 |
Cr5O12 (mp-19575) | 0.5602 | 0.025 | 2 |
VO2 (mp-776137) | 0.5849 | 0.099 | 2 |
V3(P2O7)2 (mp-32416) | 0.5114 | 0.022 | 3 |
Fe3(PO4)4 (mp-31829) | 0.4865 | 0.109 | 3 |
Co3(P2O7)2 (mp-540500) | 0.5099 | 0.029 | 3 |
Tl2Cr3O12 (mp-560926) | 0.4672 | 0.000 | 3 |
Mn3(P2O7)2 (mp-694554) | 0.5052 | 0.018 | 3 |
RbScAsO4F (mp-15865) | 0.3109 | 0.000 | 5 |
KGaPO4F (mp-9332) | 0.3297 | 0.000 | 5 |
KFePO4F (mp-19558) | 0.3504 | 0.000 | 5 |
KCrPO4F (mp-19498) | 0.3170 | 0.000 | 5 |
LiMnPO4F (mp-762774) | 0.4039 | 0.054 | 5 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.7001 | 0.040 | 6 |
Na2Gd2MgSi4(O6F)2 (mp-557538) | 0.6437 | 0.000 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.6448 | 0.018 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.7029 | 0.020 | 6 |
LiVCrP2(O4F)2 (mp-767223) | 0.6895 | 0.009 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7055 | 0.002 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points4 |
U Values-- |
PseudopotentialsVASP PAW: O P Ti_pv Tl_d |
Final Energy/Atom-7.4085 eV |
Corrected Energy-502.2330 eV
-502.2330 eV = -474.1414 eV (uncorrected energy) - 28.0916 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)