Final Magnetic Moment3.495 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.679 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.97 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbam [55] |
Hall-P 2 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 218.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 93.5 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 231.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 249.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 249.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 280.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 93.5 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 165.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 93.5 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 165.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 343.0 |
Te2Mo (mp-602) | <1 1 1> | <0 1 0> | 281.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 343.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 154.0 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 280.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 249.4 |
BN (mp-984) | <1 1 0> | <1 1 1> | 168.7 |
Al (mp-134) | <1 1 0> | <0 0 1> | 93.5 |
Al (mp-134) | <1 1 1> | <0 1 1> | 231.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 249.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 218.3 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 165.8 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 343.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 280.6 |
C (mp-66) | <1 1 1> | <0 0 1> | 249.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 343.0 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 155.9 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 187.1 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 281.7 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 280.6 |
GaP (mp-2490) | <1 1 1> | <0 1 1> | 154.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 187.1 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 165.8 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 249.4 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 1> | 231.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 280.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 249.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 124.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 154.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 165.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 249.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 249.4 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 165.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 218.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 93.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 343.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 231.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 93.5 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 231.1 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 249.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y5(In2Pd)2 (mp-980936) | 0.3825 | 0.000 | 3 |
Lu5(In2Ni)2 (mp-646321) | 0.4611 | 0.000 | 3 |
Zr5(In2Rh)2 (mp-632693) | 0.6537 | 0.000 | 3 |
Dy5(In2Ni)2 (mp-607124) | 0.3749 | 0.000 | 3 |
Mg6NbC (mp-1016630) | 0.6320 | 0.780 | 3 |
GaAu2 (mp-30380) | 0.6138 | 0.018 | 2 |
MgSi2 (mp-1073587) | 0.6500 | 0.280 | 2 |
Mg4Si3 (mp-1074350) | 0.6278 | 0.210 | 2 |
Mg2Si (mp-1074613) | 0.6174 | 0.212 | 2 |
Mg2Si (mp-1074770) | 0.6649 | 0.241 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce In_d Pt |
Final Energy/Atom-5.4800 eV |
Corrected Energy-120.5600 eV
Uncorrected energy = -120.5600 eV
Corrected energy = -120.5600 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)