Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.198 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.285 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToW2N3 + N2 |
Band Gap1.794 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3 [147] |
Hall-P 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 241.2 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 143.8 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 208.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 235.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 139.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 235.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 278.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 278.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 235.3 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 208.8 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 278.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 208.8 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 139.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 69.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 313.7 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 78.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 313.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 235.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 313.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 120.6 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 313.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 139.2 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 313.7 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 78.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 313.7 |
TiO2 (mp-2657) | <1 0 1> | <1 0 1> | 104.9 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 278.5 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 78.4 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 278.5 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 1 0> | 241.2 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 313.7 |
LaF3 (mp-905) | <1 1 0> | <1 0 0> | 278.5 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 208.8 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 278.5 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 313.7 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 235.3 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 78.4 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 156.9 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 156.9 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 1> | 209.7 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 139.2 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 139.2 |
WS2 (mp-224) | <1 1 0> | <1 1 0> | 241.2 |
C (mp-48) | <1 0 1> | <1 1 0> | 120.6 |
YAlO3 (mp-3792) | <1 0 0> | <1 1 0> | 120.6 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 235.3 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 278.5 |
CdWO4 (mp-19387) | <1 1 1> | <1 0 0> | 208.8 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 278.5 |
YAlO3 (mp-3792) | <1 1 1> | <1 1 0> | 120.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SbKr3F11 (mp-30013) | 0.5633 | 0.006 | 3 |
AsXeF7 (mp-27750) | 0.6754 | 0.000 | 3 |
CrXeF6 (mp-558341) | 0.6417 | 0.000 | 3 |
WN3F5 (mp-558743) | 0.5114 | 0.125 | 3 |
AsXe2F9 (mp-637062) | 0.6705 | 0.000 | 3 |
MgAs2(XeF5)4 (mp-555546) | 0.6201 | 0.000 | 4 |
CuSb2(XeF8)2 (mp-606617) | 0.6688 | 0.000 | 4 |
MgAs2(XeF8)2 (mp-556078) | 0.6223 | 0.000 | 4 |
SbCNCl6 (mp-570727) | 0.6375 | 0.075 | 4 |
MnH(CO)4 (mp-745016) | 0.6657 | 0.689 | 4 |
TiF4 (mp-28974) | 0.6627 | 0.000 | 2 |
MgN8 (mp-1078930) | 0.6036 | 1.057 | 2 |
CdCl4 (mp-1080124) | 0.7040 | 0.291 | 2 |
MnTeC5O6F5 (mp-650943) | 0.6255 | 0.493 | 5 |
Rb2FeC5N6O (mp-622613) | 0.6603 | 0.501 | 5 |
CSNOF5 (mp-672266) | 0.6021 | 0.247 | 5 |
ZnAs2C12(NF)12 (mp-555971) | 0.4755 | 0.318 | 5 |
Sb3C2N(OF8)2 (mp-566334) | 0.6495 | 0.078 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: W_pv N |
Final Energy/Atom-8.0181 eV |
Corrected Energy-304.6884 eV
-304.6884 eV = -304.6884 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)