Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-1.169 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 103.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 237.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 59.3 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 230.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 222.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 142.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 311.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 222.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 281.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 222.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 248.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 103.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 281.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 296.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 237.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 59.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 177.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 253.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 142.1 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 192.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 284.1 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 316.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 355.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 106.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 281.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 230.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 311.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 237.2 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 142.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 59.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 118.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 192.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 142.1 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 163.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 148.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 252.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 118.6 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 71.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 192.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 284.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 340.9 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 307.9 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 237.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 222.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 222.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 284.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 296.4 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 307.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 106.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 192.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SrZnSi (mp-9556) | 0.0512 | 0.000 | 3 |
CaAlSi (mp-3173) | 0.0500 | 0.004 | 3 |
EuPPt (mp-672290) | 0.0488 | 0.000 | 3 |
SrAsPd (mp-9743) | 0.0512 | 0.000 | 3 |
EuZnGe (mp-1009504) | 0.0485 | 0.024 | 3 |
CrB2 (mp-374) | 0.0776 | 0.089 | 2 |
CaSi2 (mp-12892) | 0.0510 | 0.078 | 2 |
EuGa2 (mp-21168) | 0.0526 | 0.045 | 2 |
LaGa2 (mp-19839) | 0.0677 | 0.000 | 2 |
EuSi2 (mp-19862) | 0.0531 | 0.011 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Eu P Pt |
Final Energy/Atom-8.4277 eV |
Corrected Energy-50.5663 eV
Uncorrected energy = -50.5663 eV
Corrected energy = -50.5663 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)