Final Magnetic Moment6.037 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.099 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.036 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGaFe3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaTe (mp-542812) | <0 0 1> | <1 1 1> | 289.6 |
MgF2 (mp-1249) | <1 1 1> | <1 0 0> | 301.0 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 234.1 |
C (mp-48) | <0 0 1> | <1 0 0> | 334.5 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 334.5 |
BN (mp-984) | <0 0 1> | <1 0 0> | 267.6 |
MoSe2 (mp-1634) | <1 1 0> | <1 0 0> | 267.6 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 167.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 167.2 |
MgAl2O4 (mp-3536) | <1 0 0> | <1 0 0> | 66.9 |
SiC (mp-11714) | <0 0 1> | <1 1 1> | 57.9 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 1 0> | 94.6 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 57.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 33.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 47.3 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 0> | 94.6 |
SiC (mp-8062) | <1 1 1> | <1 1 1> | 231.7 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 141.9 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 234.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 267.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 94.6 |
Si (mp-149) | <1 0 0> | <1 0 0> | 267.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 301.0 |
ZnO (mp-2133) | <0 0 1> | <1 0 0> | 167.2 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 133.8 |
C (mp-66) | <1 0 0> | <1 0 0> | 167.2 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 33.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 200.7 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 283.8 |
Ge (mp-32) | <1 1 0> | <1 1 0> | 47.3 |
Ge (mp-32) | <1 1 1> | <1 1 1> | 57.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 167.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 133.8 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 133.8 |
BN (mp-984) | <1 1 1> | <1 1 0> | 236.5 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 189.2 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 167.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 33.4 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 173.8 |
Ga2O3 (mp-886) | <0 1 0> | <1 1 0> | 141.9 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 141.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 47.3 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 234.1 |
Al (mp-134) | <1 1 1> | <1 0 0> | 167.2 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 57.9 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 301.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 33.4 |
LiAlO2 (mp-3427) | <1 1 1> | <1 0 0> | 267.6 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 231.7 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 0> | 133.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
135 | 142 | 142 | 0 | 0 | 0 |
142 | 135 | 142 | 0 | 0 | 0 |
142 | 142 | 135 | 0 | 0 | 0 |
0 | 0 | 0 | 132 | 0 | 0 |
0 | 0 | 0 | 0 | 132 | 0 |
0 | 0 | 0 | 0 | 0 | 132 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-91.2 | 46.8 | 46.8 | 0 | 0 | 0 |
46.8 | -91.2 | 46.8 | 0 | 0 | 0 |
46.8 | 46.8 | -91.2 | 0 | 0 | 0 |
0 | 0 | 0 | 7.6 | 0 | 0 |
0 | 0 | 0 | 0 | 7.6 | 0 |
0 | 0 | 0 | 0 | 0 | 7.6 |
Shear Modulus GV78 GPa |
Bulk Modulus KV140 GPa |
Shear Modulus GR-9 GPa |
Bulk Modulus KR140 GPa |
Shear Modulus GVRH34 GPa |
Bulk Modulus KVRH140 GPa |
Elastic Anisotropy-46.04 |
Poisson's Ratio0.39 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
GdSnRh2 (mp-866089) | 0.0002 | 1.204 | 3 |
PuCdRh2 (mp-862738) | 0.0002 | 0.149 | 3 |
TiInCo2 (mp-865548) | 0.0002 | 0.000 | 3 |
TiInPd2 (mp-866168) | 0.0003 | 0.000 | 3 |
SmInRh2 (mp-867978) | 0.0002 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0038 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0038 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0038 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0038 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0038 | 0.000 | 4 |
MnS (mp-850100) | 0.0038 | 0.501 | 2 |
Mg3Pa (mp-978291) | 0.0038 | 0.353 | 2 |
MgRe3 (mp-977283) | 0.0038 | 0.269 | 2 |
Rb3Tc (mp-974820) | 0.0002 | 1.260 | 2 |
NaEr3 (mp-976405) | 0.0038 | 0.318 | 2 |
Br (mp-673171) | 0.0038 | 0.630 | 1 |
Ti (mp-73) | 0.0038 | 0.112 | 1 |
I (mp-684663) | 0.0038 | 0.446 | 1 |
Cr (mp-90) | 0.0038 | 0.000 | 1 |
Bi (mp-568610) | 0.0038 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ga_d Fe_pv |
Final Energy/Atom-7.2090 eV |
Corrected Energy-28.8360 eV
-28.8360 eV = -28.8360 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)