Final Magnetic Moment0.043 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.369 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.050 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSbP2O7 + P2O5 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 265.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 331.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 199.1 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 331.9 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 129.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 199.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 265.5 |
InAs (mp-20305) | <1 1 1> | <1 0 -1> | 129.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 199.1 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 138.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 265.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 199.1 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 138.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 199.1 |
BN (mp-984) | <0 0 1> | <1 0 1> | 174.9 |
BN (mp-984) | <1 1 1> | <1 0 0> | 138.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 265.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 265.5 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 259.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 265.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 132.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 66.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 331.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 331.9 |
TiO2 (mp-2657) | <1 1 1> | <1 0 1> | 174.9 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 199.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 199.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 199.1 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 259.4 |
Ni (mp-23) | <1 1 1> | <1 0 -1> | 129.7 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 138.9 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 331.9 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 -1> | 259.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 174.9 |
C (mp-66) | <1 0 0> | <0 0 1> | 265.5 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 265.5 |
MoSe2 (mp-1634) | <1 1 1> | <0 0 1> | 265.5 |
C (mp-66) | <1 1 0> | <0 0 1> | 265.5 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 265.5 |
Si (mp-149) | <1 1 1> | <0 0 1> | 199.1 |
Au (mp-81) | <1 0 0> | <1 0 -1> | 259.4 |
Au (mp-81) | <1 1 1> | <0 0 1> | 265.5 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 331.9 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 265.5 |
WSe2 (mp-1821) | <1 1 0> | <1 0 -1> | 259.4 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 265.5 |
ZrO2 (mp-2858) | <1 1 1> | <0 0 1> | 265.5 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 265.5 |
CaCO3 (mp-3953) | <1 0 0> | <1 0 -1> | 259.4 |
CaCO3 (mp-3953) | <1 0 1> | <0 0 1> | 265.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BiP2O7 (mp-26658) | 0.7245 | 0.080 | 3 |
Y2P4O13 (mp-30321) | 0.4894 | 0.003 | 3 |
Bi(PO3)4 (mp-684096) | 0.2117 | 0.046 | 3 |
K2Si4O9 (mp-558603) | 0.6728 | 0.000 | 3 |
Sn(PO3)3 (mp-26172) | 0.5920 | 0.088 | 3 |
Cs3P7Pb2O21 (mp-572271) | 0.5170 | 0.000 | 4 |
KUP3O11 (mp-557505) | 0.5867 | 0.000 | 4 |
KYb(PO3)4 (mp-616490) | 0.2744 | 0.000 | 4 |
SmP4HO12 (mp-542237) | 0.4865 | 0.000 | 4 |
BiP4HO12 (mp-24348) | 0.4714 | 0.000 | 4 |
Rb2EuGa(SiO3)4 (mp-684467) | 0.6907 | 0.129 | 5 |
Rb2TbGa(SiO3)4 (mp-558318) | 0.6858 | 0.000 | 5 |
Rb2GdGa(SiO3)4 (mp-555485) | 0.6716 | 0.000 | 5 |
CsUGa(PO5)2 (mp-559852) | 0.6561 | 0.000 | 5 |
K2CeAl(SiO3)4 (mp-1019774) | 0.6565 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sb P O |
Final Energy/Atom-6.8828 eV |
Corrected Energy-501.7374 eV
-501.7374 eV = -468.0275 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)