Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.594 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.044 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiPO3 + LiSn2(PO3)5 |
Band Gap4.508 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 208.1 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 312.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 156.1 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 242.0 |
AlN (mp-661) | <0 0 1> | <0 1 -1> | 168.3 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 243.4 |
AlN (mp-661) | <1 1 1> | <1 -1 0> | 254.6 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 321.3 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 252.7 |
GaN (mp-804) | <1 0 0> | <0 1 -1> | 168.3 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 243.4 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 267.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 325.2 |
GaAs (mp-2534) | <1 0 0> | <1 -1 1> | 237.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 -1> | 336.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 -1> | 294.8 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 252.7 |
KCl (mp-23193) | <1 0 0> | <0 1 -1> | 280.5 |
KCl (mp-23193) | <1 1 1> | <0 1 -1> | 280.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 -1> | 221.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 -1 0> | 318.3 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 216.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 156.1 |
InAs (mp-20305) | <1 1 1> | <0 1 -1> | 336.6 |
ZnSe (mp-1190) | <1 0 0> | <1 -1 1> | 237.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 -1> | 336.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 -1> | 112.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 271.0 |
CdS (mp-672) | <1 0 0> | <1 1 -1> | 147.4 |
CdS (mp-672) | <1 0 1> | <0 1 -1> | 224.4 |
CdS (mp-672) | <1 1 0> | <1 -1 1> | 237.6 |
CdS (mp-672) | <1 1 1> | <1 -1 0> | 318.3 |
LiF (mp-1138) | <1 0 0> | <0 1 -1> | 168.3 |
LiF (mp-1138) | <1 1 0> | <1 -1 1> | 237.6 |
LiF (mp-1138) | <1 1 1> | <1 -1 1> | 316.8 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 267.8 |
YVO4 (mp-19133) | <1 1 0> | <1 -1 1> | 316.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 260.1 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 304.3 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 267.8 |
BN (mp-984) | <0 0 1> | <1 -1 1> | 158.4 |
BN (mp-984) | <1 1 1> | <0 1 -1> | 280.5 |
MoS2 (mp-1434) | <1 0 1> | <1 -1 -1> | 263.4 |
Al (mp-134) | <1 0 0> | <0 1 -1> | 112.2 |
Al (mp-134) | <1 1 1> | <1 -1 0> | 318.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 -1 0> | 254.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 -1 0> | 127.3 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 261.3 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 208.1 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 -1> | 182.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sn3(AsO4)4 (mvc-6184) | 0.6999 | 0.182 | 3 |
Fe3(AsO4)4 (mvc-6284) | 0.7383 | 0.369 | 3 |
Co3(AsO4)4 (mvc-6165) | 0.6113 | 0.214 | 3 |
Li4Mn(PO3)6 (mp-782696) | 0.5420 | 0.064 | 4 |
Li3Sn(PO3)6 (mp-673096) | 0.4641 | 0.087 | 4 |
Li2SnP2O7 (mp-761841) | 0.6293 | 0.034 | 4 |
Li4V(PO3)6 (mp-762973) | 0.5889 | 0.071 | 4 |
Li6Sn5(P2O7)4 (mp-765227) | 0.5841 | 0.061 | 4 |
Li4MnP6(H4O11)2 (mp-780144) | 0.7493 | 0.055 | 5 |
Li4CrP6(H4O11)2 (mp-775207) | 0.7250 | 0.094 | 5 |
Li7MnP4O14F (mp-762708) | 0.7446 | 0.151 | 5 |
Li2SbP(OF3)2 (mp-776357) | 0.6946 | 0.088 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sn_d P O |
Final Energy/Atom-6.7504 eV |
Corrected Energy-208.4021 eV
-208.4021 eV = -195.7609 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)