Final Magnetic Moment0.436 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.938 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.062 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu3(PO4)2 + Li2CuP2O7 + CuO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 328.5 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 1> | 142.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 280.5 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 280.5 |
GaN (mp-804) | <1 0 0> | <1 -1 -1> | 101.6 |
GaN (mp-804) | <1 0 1> | <0 1 -1> | 207.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 210.0 |
SiO2 (mp-6930) | <1 0 1> | <1 -1 1> | 105.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 104.7 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 328.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 287.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 -1> | 276.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 -1 -1> | 203.3 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 197.1 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 287.2 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 209.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 210.0 |
Te2Mo (mp-602) | <1 0 0> | <1 -1 0> | 259.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 287.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 287.2 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 280.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 287.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 197.1 |
Al (mp-134) | <1 0 0> | <0 1 -1> | 276.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 328.5 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 1> | 142.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 -1> | 90.2 |
TeO2 (mp-2125) | <0 0 1> | <1 -1 0> | 259.2 |
MgO (mp-1265) | <1 1 0> | <0 1 -1> | 207.2 |
TiO2 (mp-2657) | <1 0 0> | <0 1 -1> | 69.1 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 262.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 229.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 197.1 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 210.4 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 262.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 287.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 328.5 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 197.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 287.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 287.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 -1> | 276.2 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 -1> | 203.3 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 142.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 287.2 |
Te2W (mp-22693) | <0 0 1> | <1 -1 -1> | 203.3 |
YVO4 (mp-19133) | <1 1 0> | <1 -1 -1> | 203.3 |
MoS2 (mp-1434) | <0 0 1> | <1 -1 -1> | 203.3 |
MoS2 (mp-1434) | <1 0 0> | <1 -1 -1> | 203.3 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 287.2 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 229.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu4(PO4)3 (mp-673151) | 0.3101 | 0.039 | 3 |
Mn3(PO4)2 (mp-770563) | 0.4507 | 0.015 | 3 |
Fe3(PO4)2 (mp-636647) | 0.4230 | 0.000 | 3 |
Ni3(PO4)2 (mp-771911) | 0.4405 | 0.192 | 3 |
Cr4(PO4)3 (mp-774538) | 0.4712 | 0.324 | 3 |
Li3Cr3(PO4)4 (mp-780336) | 0.4422 | 0.081 | 4 |
Li3V3(PO4)4 (mp-763450) | 0.4540 | 0.150 | 4 |
Li3Fe3(PO4)4 (mp-31797) | 0.3626 | 0.049 | 4 |
LiFe4(PO4)3 (mp-762674) | 0.3759 | 0.539 | 4 |
KCu4(PO4)3 (mp-559343) | 0.4417 | 0.023 | 4 |
LiFe3SiPO8 (mp-743761) | 0.5957 | 0.221 | 5 |
Na2Li2V3P2O13 (mp-853239) | 0.6072 | 0.061 | 5 |
K2Mn2Zn4Si4O15 (mp-567173) | 0.6198 | 0.004 | 5 |
NaCa2SiO4F (mp-684821) | 0.6948 | 0.291 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv P O |
Final Energy/Atom-6.2124 eV |
Corrected Energy-265.3512 eV
-265.3512 eV = -248.4962 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)