Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.914 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.017 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToIn2S3 |
Band Gap1.610 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 319.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 295.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 169.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 319.3 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 228.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 -1> | 216.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 319.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 196.7 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 168.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 228.0 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 288.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 228.0 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 168.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 98.3 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 287.1 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 319.3 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 252.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 45.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 252.4 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 273.7 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 228.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 45.6 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 228.0 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 319.3 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 228.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 169.6 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 168.3 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 182.4 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 273.7 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 319.3 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 168.3 |
Al (mp-134) | <1 1 0> | <0 1 0> | 45.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 -1> | 216.8 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 273.7 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 182.4 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 319.3 |
BN (mp-984) | <1 0 1> | <0 1 0> | 182.4 |
BN (mp-984) | <1 1 1> | <0 1 0> | 319.3 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 168.3 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 -1> | 295.0 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 98.3 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 252.4 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 252.4 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 319.3 |
C (mp-66) | <1 0 0> | <1 0 0> | 252.4 |
C (mp-66) | <1 1 0> | <0 1 1> | 288.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 319.3 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 273.7 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 319.3 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 136.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al(CuSe2)3 (mvc-11839) | 0.3968 | 0.202 | 3 |
Al(CuS2)3 (mvc-14816) | 0.2973 | 0.298 | 3 |
Ga3Te3As (mp-675954) | 0.3248 | 0.027 | 3 |
In3AsSe3 (mp-675930) | 0.3172 | 0.019 | 3 |
Cd(Ga3Te5)2 (mp-36641) | 0.2766 | 0.004 | 3 |
CuAs4S3Cl (mp-558199) | 0.6575 | 0.004 | 4 |
Ga2Te3 (mp-38970) | 0.1469 | 0.000 | 2 |
Ga2S3 (mp-32616) | 0.1329 | 0.001 | 2 |
Al2Se3 (mp-11674) | 0.3031 | 0.000 | 2 |
Ga2S3 (mp-539) | 0.3053 | 0.000 | 2 |
Ga2Se3 (mp-1340) | 0.1384 | 0.000 | 2 |
Explore more synthesis descriptions for materials of composition In2S3.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: In_d S |
Final Energy/Atom-4.0982 eV |
Corrected Energy-44.9625 eV
-44.9625 eV = -40.9818 eV (uncorrected energy) - 3.9808 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)