Final Magnetic Moment0.097 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom0.040 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.204 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe3N |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP312 [149] |
HallP 3 2 |
Point Group32 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 75.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 356.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 338.1 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 75.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 169.0 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 139.0 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 160.5 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 56.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 356.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 169.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 244.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 300.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 300.5 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 300.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 75.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 247.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 225.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 225.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 139.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 187.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 131.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 244.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 225.4 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 247.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 93.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 375.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 169.0 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 139.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 56.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 93.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 300.5 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 300.5 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 75.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 131.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 131.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 356.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 75.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 262.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 356.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 225.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 225.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 131.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 244.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 169.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 131.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 169.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 75.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 319.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 300.5 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 319.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
312 | 141 | 142 | 0 | 3 | 0 |
141 | 312 | 142 | 0 | -3 | 0 |
142 | 142 | 323 | 0 | 0 | 0 |
0 | 0 | 0 | 104 | 0 | -3 |
3 | -3 | 0 | 0 | 104 | 0 |
0 | 0 | 0 | -3 | 0 | 86 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4.4 | -1.4 | -1.3 | 0 | -0.2 | 0 |
-1.4 | 4.4 | -1.3 | 0 | 0.2 | 0 |
-1.3 | -1.3 | 4.3 | 0 | 0 | 0 |
0 | 0 | 0 | 9.6 | 0 | 0.3 |
-0.2 | 0.2 | 0 | 0 | 9.6 | 0 |
0 | 0 | 0 | 0.3 | 0 | 11.7 |
Shear Modulus GV94 GPa |
Bulk Modulus KV200 GPa |
Shear Modulus GR93 GPa |
Bulk Modulus KR200 GPa |
Shear Modulus GVRH93 GPa |
Bulk Modulus KVRH200 GPa |
Elastic Anisotropy0.05 |
Poisson's Ratio0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
PdPtF6 (mp-8547) | 0.3926 | 0.000 | 3 |
ThSnI6 (mp-28815) | 0.2491 | 0.021 | 3 |
ThPbI6 (mp-505148) | 0.3161 | 0.033 | 3 |
NiPtF6 (mp-612185) | 0.4588 | 0.000 | 3 |
LiAuF6 (mp-1079483) | 0.4451 | 0.000 | 3 |
Fe3N (mp-906903) | 0.0437 | 0.000 | 2 |
Ni3N (mp-2033) | 0.0575 | 0.000 | 2 |
Fe3C (mp-13154) | 0.0980 | 0.055 | 2 |
Pd3N (mp-1079760) | 0.0700 | 0.222 | 2 |
Fe3N (mp-1804) | 0.0366 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Fe_pv N |
Final Energy/Atom-8.3001 eV |
Corrected Energy-265.6037 eV
-265.6037 eV = -265.6037 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)