Final Magnetic Moment3.997 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.946 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom< 0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCe5O9 + CeO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 216.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 268.1 |
GaN (mp-804) | <0 0 1> | <0 1 -1> | 205.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 216.9 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 290.8 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 143.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 216.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 268.1 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 290.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 268.1 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 290.8 |
BN (mp-984) | <1 1 0> | <0 1 0> | 260.3 |
BN (mp-984) | <1 1 1> | <1 0 0> | 268.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 216.9 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 289.2 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 268.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 216.9 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 289.2 |
TeO2 (mp-2125) | <0 1 0> | <1 -1 0> | 203.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 289.2 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 260.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 216.9 |
TiO2 (mp-2657) | <0 0 1> | <1 -1 -1> | 236.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 178.7 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 0> | 173.5 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 216.9 |
Mg (mp-153) | <1 1 0> | <1 0 -1> | 290.8 |
LaF3 (mp-905) | <1 0 0> | <1 -1 1> | 262.0 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 260.3 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 -1> | 290.8 |
Au (mp-81) | <1 1 1> | <0 0 1> | 216.9 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 261.0 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 216.9 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 1> | 122.4 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 144.6 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 268.1 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 268.1 |
BaTiO3 (mp-5986) | <1 1 1> | <1 -1 1> | 262.0 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 289.2 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 289.2 |
SiC (mp-11714) | <1 0 1> | <0 1 0> | 260.3 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 216.9 |
C (mp-48) | <0 0 1> | <0 0 1> | 289.2 |
CdWO4 (mp-19387) | <0 1 0> | <1 -1 -1> | 236.5 |
CdWO4 (mp-19387) | <0 1 1> | <0 1 -1> | 205.2 |
CdWO4 (mp-19387) | <1 1 0> | <0 1 -1> | 205.2 |
TiO2 (mp-390) | <1 1 1> | <0 0 1> | 216.9 |
ZnO (mp-2133) | <0 0 1> | <1 0 0> | 178.7 |
ZnO (mp-2133) | <1 0 1> | <0 1 0> | 260.3 |
MgAl2O4 (mp-3536) | <1 1 0> | <0 0 1> | 289.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ce6Th4O19 (mp-676287) | 0.2232 | 0.000 | 3 |
Ce6Y2O15 (mp-758094) | 0.2313 | 0.016 | 3 |
Y10U4O27 (mp-685633) | 0.4381 | 0.000 | 3 |
Yb6U3O17 (mp-675015) | 0.3758 | 0.000 | 3 |
Ce4ThO9 (mp-753456) | 0.4024 | 0.075 | 3 |
Ce13O24 (mp-684627) | 0.3788 | 0.004 | 2 |
U6O11 (mp-761153) | 0.3632 | 0.043 | 2 |
Pr6O11 (mp-559771) | 0.2764 | 0.074 | 2 |
Ce5O9 (mp-32613) | 0.3408 | 0.007 | 2 |
Ce11O20 (mp-505619) | 0.3740 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce O |
Final Energy/Atom-8.7772 eV |
Corrected Energy-452.5575 eV
-452.5575 eV = -430.0842 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)