Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.662 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.018 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNd10Se19 |
Band Gap0.003 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 238.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 238.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 238.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 238.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 238.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 317.7 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 173.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 238.3 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 317.7 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 173.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 317.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 238.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 317.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 173.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 317.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 317.7 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 317.7 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 156.4 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 238.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 238.3 |
Au (mp-81) | <1 0 0> | <0 1 1> | 173.9 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 317.7 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 238.3 |
C (mp-48) | <1 1 1> | <0 0 1> | 238.3 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 317.7 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 238.3 |
ZrO2 (mp-2858) | <1 0 1> | <0 1 1> | 173.9 |
ZrO2 (mp-2858) | <1 1 -1> | <0 0 1> | 317.7 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 158.9 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 158.9 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 317.7 |
ZnO (mp-2133) | <1 0 0> | <0 1 1> | 173.9 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 158.9 |
GaTe (mp-542812) | <0 0 1> | <0 1 0> | 156.4 |
GaTe (mp-542812) | <1 0 -1> | <0 1 0> | 156.4 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 238.3 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 238.3 |
LiAlO2 (mp-3427) | <1 0 1> | <0 1 1> | 173.9 |
LiAlO2 (mp-3427) | <1 1 0> | <0 0 1> | 317.7 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 79.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KNd3Te8 (mp-669359) | 0.7028 | 0.000 | 3 |
BaThTe4 (mp-1095218) | 0.5251 | 0.009 | 3 |
Ba3ThSe7 (mp-1095255) | 0.6004 | 0.000 | 3 |
BaUTe4 (mp-1095338) | 0.6329 | 0.079 | 3 |
Ti20(Sb3Se)3 (mp-530251) | 0.7448 | 0.009 | 3 |
La10Se19 (mp-8866) | 0.5947 | 0.000 | 2 |
Sm5Se9 (mp-684959) | 0.3603 | 0.046 | 2 |
Pr10Se19 (mp-14613) | 0.5603 | 0.000 | 2 |
Nd10Se19 (mp-14650) | 0.5595 | 0.000 | 2 |
Sm10Se19 (mp-29832) | 0.5608 | 0.002 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Se |
Final Energy/Atom-5.5964 eV |
Corrected Energy-324.5915 eV
-324.5915 eV = -324.5915 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)