Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.153 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.030 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNbO2F |
Band Gap1.951 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 268.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 313.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 197.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 295.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 313.3 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 98.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 223.8 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 197.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 164.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 313.3 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 295.7 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 263.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 98.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 295.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 223.8 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 98.6 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 295.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 216.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 98.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 313.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 134.3 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 98.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 134.3 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 295.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 263.6 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 268.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 223.8 |
BN (mp-984) | <1 1 0> | <1 0 0> | 131.8 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 295.7 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 134.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 134.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 268.5 |
Al (mp-134) | <1 0 0> | <0 1 0> | 98.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 223.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 268.5 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 98.6 |
TeO2 (mp-2125) | <1 0 0> | <0 1 1> | 216.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 268.5 |
Al (mp-134) | <1 1 0> | <0 1 0> | 295.7 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 313.3 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 295.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 179.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 223.8 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 98.6 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 164.6 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 0> | 164.6 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 197.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 313.3 |
C (mp-66) | <1 1 0> | <0 1 0> | 197.2 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 263.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mo5(O4F)3 (mp-705844) | 0.2858 | 0.001 | 3 |
WO2F (mp-767155) | 0.3149 | 0.053 | 3 |
NbO2F (mp-756632) | 0.2857 | 0.047 | 3 |
NbCrF6 (mp-611999) | 0.3214 | 0.034 | 3 |
NbCrF6 (mp-554813) | 0.3328 | 0.034 | 3 |
CoAg3(CN)6 (mp-6573) | 0.5811 | 0.236 | 4 |
ErCo(CN)6 (mp-6185) | 0.6832 | 0.034 | 4 |
FeAg3(CN)6 (mp-568663) | 0.5817 | 0.307 | 4 |
WO3 (mp-636289) | 0.3831 | 0.002 | 2 |
WO3 (mp-510417) | 0.4074 | 0.001 | 2 |
WO3 (mp-566278) | 0.3812 | 0.000 | 2 |
WO3 (mp-19443) | 0.4515 | 0.000 | 2 |
WO3 (mp-19033) | 0.4637 | 0.001 | 2 |
Cs2LiCr(CN)6 (mp-570502) | 0.6783 | 0.135 | 5 |
Cs2LiCr(CN)6 (mp-540847) | 0.6511 | 0.182 | 5 |
K2NaAg3(CN)6 (mp-6855) | 0.7019 | 0.207 | 5 |
Rb2LiCo(CN)6 (mp-15182) | 0.7499 | 0.101 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv O F |
Final Energy/Atom-8.1564 eV |
Corrected Energy-206.7687 eV
Uncorrected energy = -195.7527 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Composition-based energy adjustment (-0.462 eV/atom x 6.0 atoms) = -2.7720 eV
Corrected energy = -206.7687 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)