Final Magnetic Moment3.916 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.408 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 1> | <0 0 1> | 191.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 60.2 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 100.9 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 301.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 127.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 255.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 180.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 180.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 318.8 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 216.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 180.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 191.3 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 144.1 |
CeO2 (mp-20194) | <1 1 1> | <1 0 -1> | 216.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 180.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 201.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 216.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 180.6 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 100.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 255.1 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 318.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 60.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 318.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 180.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 301.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 191.3 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 318.8 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 288.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 318.8 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 288.2 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 301.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 318.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 258.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 301.0 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 318.8 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 180.6 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 240.8 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 -1> | 72.1 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 318.8 |
Al (mp-134) | <1 1 0> | <1 0 0> | 180.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 191.3 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 255.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 191.3 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 318.8 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 301.0 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 191.3 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 180.6 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 180.6 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 191.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 191.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ce6Th4O19 (mp-676287) | 0.3887 | 0.000 | 3 |
Li14Mn2S9 (mp-756198) | 0.5649 | 0.000 | 3 |
Ce6Y2O15 (mp-758094) | 0.4034 | 0.016 | 3 |
Y10U4O27 (mp-685633) | 0.5452 | 0.000 | 3 |
Ce4ThO9 (mp-753456) | 0.4798 | 0.075 | 3 |
Ce17O32 (mp-673643) | 0.3758 | 0.000 | 2 |
U6O11 (mp-761153) | 0.4987 | 0.043 | 2 |
Pr6O11 (mp-559771) | 0.3689 | 0.074 | 2 |
Ce5O9 (mp-32613) | 0.5224 | 0.007 | 2 |
Ce11O20 (mp-505619) | 0.5448 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Yb_2 U O |
Final Energy/Atom-7.8422 eV |
Corrected Energy-215.5755 eV
Uncorrected energy = -203.8965 eV
Composition-based energy adjustment (-0.687 eV/atom x 17.0 atoms) = -11.6790 eV
Corrected energy = -215.5755 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)