material

Cu2SiTe3

ID:

mp-675120

DOI:

10.17188/1282593


Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.285 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.60 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.168 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cc [9]
Hall
C 2yc
Point Group
m
Crystal System
monoclinic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.003 184.9
WS2 (mp-224) <0 0 1> <0 0 1> 0.003 184.9
PbS (mp-21276) <1 0 0> <0 1 0> 0.006 251.8
InP (mp-20351) <1 1 1> <0 0 1> 0.006 184.9
Mg (mp-153) <0 0 1> <0 0 1> 0.007 184.9
BaTiO3 (mp-5986) <1 1 0> <1 0 -1> 0.008 214.5
Mg (mp-153) <1 0 1> <1 0 1> 0.015 150.8
CdS (mp-672) <0 0 1> <0 0 1> 0.018 92.5
LiGaO2 (mp-5854) <0 1 1> <1 0 -1> 0.019 214.5
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.025 184.9
YAlO3 (mp-3792) <1 1 1> <0 1 0> 0.032 251.8
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.039 150.8
AlN (mp-661) <1 0 1> <0 1 0> 0.040 251.8
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.047 277.4
Bi2Se3 (mp-541837) <1 0 0> <0 1 0> 0.049 251.8
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.059 92.5
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.087 92.5
PbS (mp-21276) <1 1 1> <0 0 1> 0.088 184.9
MgO (mp-1265) <1 0 0> <1 0 -1> 0.090 107.2
InP (mp-20351) <1 0 0> <0 1 0> 0.094 251.8
C (mp-66) <1 1 0> <0 1 0> 0.099 201.4
MgO (mp-1265) <1 1 1> <0 1 0> 0.118 251.8
GaN (mp-804) <1 0 1> <0 1 0> 0.130 251.8
LaF3 (mp-905) <1 1 0> <0 0 1> 0.133 92.5
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.139 92.5
YVO4 (mp-19133) <1 0 1> <0 0 1> 0.140 277.4
LaF3 (mp-905) <0 0 1> <0 0 1> 0.142 92.5
CdWO4 (mp-19387) <1 0 0> <0 1 0> 0.145 251.8
Al2O3 (mp-1143) <1 0 1> <0 1 0> 0.151 201.4
MgO (mp-1265) <1 1 0> <0 1 0> 0.158 50.4
C (mp-48) <0 0 1> <0 1 0> 0.163 251.8
Fe3O4 (mp-19306) <1 0 0> <1 0 -1> 0.164 214.5
Cu (mp-30) <1 1 0> <0 1 0> 0.229 151.1
Ni (mp-23) <1 1 0> <0 1 0> 0.234 302.2
Fe3O4 (mp-19306) <1 1 0> <0 1 0> 0.257 100.7
GaTe (mp-542812) <0 0 1> <0 1 0> 0.260 151.1
ZnO (mp-2133) <1 0 1> <0 1 0> 0.264 251.8
Au (mp-81) <1 1 0> <0 1 0> 0.277 50.4
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.279 277.4
LaF3 (mp-905) <1 0 1> <0 0 1> 0.281 277.4
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.320 277.4
Ni (mp-23) <1 1 1> <0 1 0> 0.326 151.1
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.338 277.4
KTaO3 (mp-3614) <1 1 0> <0 1 0> 0.360 201.4
SiO2 (mp-6930) <1 0 0> <0 1 0> 0.369 302.2
SiC (mp-8062) <1 1 0> <0 0 1> 0.380 277.4
AlN (mp-661) <1 1 0> <0 1 0> 0.389 302.2
GaTe (mp-542812) <1 0 -1> <0 1 0> 0.406 151.1
Ag (mp-124) <1 1 0> <0 1 0> 0.408 50.4
SiO2 (mp-6930) <0 0 1> <0 1 0> 0.409 151.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
94 30 29 0 0 0
30 94 34 0 8 0
29 34 94 0 -8 0
0 0 0 28 0 8
0 8 -8 0 21 0
0 0 0 8 0 21
Compliance Tensor Sij (10-12Pa-1)
12.4 -3 -2.8 0 0.1 0
-3 14 -4.8 0 -7.3 0
-2.8 -4.8 13.9 0 7.1 0
0 0 0 39.4 0 -14.1
0.1 -7.3 7.1 0 54.2 0
0 0 0 -14.1 0 52.2
Shear Modulus GV
27 GPa
Bulk Modulus KV
52 GPa
Shear Modulus GR
23 GPa
Bulk Modulus KR
52 GPa
Shear Modulus GVRH
25 GPa
Bulk Modulus KVRH
52 GPa
Elastic Anisotropy
0.66
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
In2AsSe (mp-676682) 0.0480 0.132 3
Cu2GeSe3 (mp-677105) 0.0359 0.005 3
Cu3AsSe4 (mp-675626) 0.0585 0.000 3
Cu2GeS3 (mp-15252) 0.0480 0.000 3
Ag2SnSe3 (mp-1096812) 0.0605 0.000 3
GaFe2AgTe4 (mp-1079848) 0.0777 0.216 4
ZnCu2GeS4 (mp-6408) 0.0771 0.000 4
MnCu2SnS4 (mp-986979) 0.0756 0.000 4
ZnCu2SiTe4 (mp-1078498) 0.0693 0.000 4
ZnCu2GeTe4 (mp-12854) 0.0752 0.004 4
BeP2 (mp-27148) 0.0579 0.000 2
CuI (mp-673245) 0.0975 0.008 2
ZnTe (mp-571195) 0.1068 0.004 2
BC7 (mp-1095030) 0.1157 0.280 2
SiGe (mp-1096549) 0.0843 0.053 2
Sn (mp-949028) 0.1530 0.030 1
Si (mp-971662) 0.1551 0.064 1
Si (mp-149) 0.1780 0.000 1
Sn (mp-117) 0.1780 0.000 1
Ge (mp-32) 0.1780 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cu_pv Si Te
Final Energy/Atom
-3.9158 eV
Corrected Energy
-49.5219 eV
Uncorrected energy = -46.9899 eV Composition-based energy adjustment (-0.422 eV/atom x 6.0 atoms) = -2.5320 eV Corrected energy = -49.5219 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • Ordering of Disordered Crystal

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)