Final Magnetic Moment7.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.339 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.586 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BN (mp-984) | <0 0 1> | <0 1 0> | 293.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 214.9 |
BN (mp-984) | <1 1 0> | <0 1 0> | 176.1 |
BN (mp-984) | <1 1 1> | <0 1 0> | 293.4 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 214.9 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 234.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 293.4 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 176.3 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 216.4 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 293.4 |
SiC (mp-7631) | <1 1 0> | <0 1 0> | 234.7 |
SiC (mp-7631) | <1 1 1> | <0 1 0> | 234.7 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 214.9 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 214.9 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 234.7 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 -1> | 124.2 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 234.7 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 214.9 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 293.4 |
TiO2 (mp-2657) | <1 0 0> | <1 0 -1> | 124.2 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 293.4 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 0> | 176.1 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 0> | 293.4 |
GaP (mp-2490) | <1 1 0> | <0 1 0> | 176.1 |
GaP (mp-2490) | <1 1 1> | <1 0 0> | 107.4 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 0> | 176.1 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 176.1 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 0> | 293.4 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 234.7 |
InSb (mp-20012) | <1 0 0> | <1 0 1> | 176.3 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 216.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 214.9 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 176.1 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 107.4 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 214.9 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 293.4 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 214.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 176.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 176.1 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 293.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 293.4 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 248.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 176.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 185.8 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 293.4 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 214.9 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 214.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 -1> | 137.3 |
NdGaO3 (mp-3196) | <0 1 0> | <0 1 0> | 176.1 |
NdGaO3 (mp-3196) | <1 0 0> | <0 1 0> | 176.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3FeF6 (mp-776784) | 0.4302 | 0.065 | 3 |
Li3ScCl6 (mp-686004) | 0.1894 | 0.012 | 3 |
Li3ErBr6 (mp-37873) | 0.1996 | 0.003 | 3 |
Li3InCl6 (mp-676109) | 0.2890 | 0.000 | 3 |
Li3FeF6 (mp-777475) | 0.4136 | 0.198 | 3 |
Li2Mn3(FeO4)3 (mp-767665) | 0.4313 | 0.095 | 4 |
Li2Mn3Cr3O12 (mp-850956) | 0.4149 | 0.075 | 4 |
Li2Ti3V3O12 (mp-763640) | 0.4027 | 0.091 | 4 |
LiAl2FeO6 (mp-770071) | 0.4626 | 0.130 | 4 |
LiV2CrO6 (mp-849360) | 0.4574 | 0.107 | 4 |
Ho2Se3 (mp-9824) | 0.1867 | 0.000 | 2 |
Sc2S3 (mp-684969) | 0.2163 | 0.004 | 2 |
Sc2S3 (mp-401) | 0.1931 | 0.000 | 2 |
Er2Te3 (mp-14643) | 0.2648 | 0.000 | 2 |
Er2Se3 (mp-209) | 0.1843 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Gd I |
Final Energy/Atom-4.0547 eV |
Corrected Energy-42.8207 eV
Uncorrected energy = -40.5467 eV
Composition-based energy adjustment (-0.379 eV/atom x 6.0 atoms) = -2.2740 eV
Corrected energy = -42.8207 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)