Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.693 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.111 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTl2CuF4 + TlF + Cu |
Band Gap1.777 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 236.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 355.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 355.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 276.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 276.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 315.9 |
CeO2 (mp-20194) | <1 0 0> | <0 1 -1> | 264.9 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 142.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 315.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 39.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 276.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 157.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 197.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 315.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 315.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 276.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 315.9 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 260.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 355.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 315.9 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 130.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 276.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 197.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 315.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 157.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 276.4 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 276.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 197.4 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 260.1 |
Ag (mp-124) | <1 1 0> | <0 1 -1> | 264.9 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 130.1 |
MoS2 (mp-1434) | <1 0 1> | <0 1 -1> | 132.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 236.9 |
BN (mp-984) | <1 1 1> | <0 0 1> | 236.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 355.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 276.4 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 315.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 355.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 315.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 315.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 236.9 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 355.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 236.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 236.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 236.9 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 276.4 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 236.9 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 197.4 |
C (mp-66) | <1 1 0> | <0 0 1> | 197.4 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 236.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hg2ClO (mp-636805) | 0.4842 | 0.030 | 3 |
Zr2Cr2F3 (mp-690241) | 0.6761 | 0.950 | 3 |
Sb4Cl2O5 (mp-23419) | 0.6181 | 0.000 | 3 |
Sb4Br2O5 (mp-27700) | 0.6848 | 0.000 | 3 |
Tl2CN2 (mp-570443) | 0.6358 | 0.000 | 3 |
HgHOF (mp-23844) | 0.6995 | 0.000 | 4 |
TlAg(CN)2 (mp-621981) | 0.7096 | 0.253 | 4 |
TlAu(CN)2 (mp-569173) | 0.7049 | 0.156 | 4 |
K3NaFeCl6 (mp-690672) | 0.6484 | 0.415 | 4 |
GeF2 (mp-1095292) | 0.7458 | 0.017 | 2 |
HgCSNCl (mp-559882) | 0.7380 | 0.170 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d Cu_pv F |
Final Energy/Atom-3.8735 eV |
Corrected Energy-147.7617 eV
Uncorrected energy = -139.4457 eV
Composition-based energy adjustment (-0.462 eV/atom x 18.0 atoms) = -8.3160 eV
Corrected energy = -147.7617 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)