Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.749 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.043 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToIrSe2 + NbSe2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 -1> | 236.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 316.5 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 316.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 316.5 |
GaN (mp-804) | <0 0 1> | <1 -1 -1> | 242.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 253.2 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 211.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 236.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 316.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 316.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 316.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 253.2 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 237.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 316.5 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 253.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 316.5 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 189.9 |
YVO4 (mp-19133) | <1 0 1> | <0 1 -1> | 290.8 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 316.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 -1> | 290.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 316.5 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 -1> | 290.8 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 223.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 316.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 316.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 189.9 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 316.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 316.4 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 316.4 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 -1> | 290.8 |
LiTaO3 (mp-3666) | <1 0 1> | <1 0 0> | 223.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 189.9 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 253.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 316.5 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 316.5 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 -1> | 236.5 |
Mg (mp-153) | <1 0 1> | <1 -1 -1> | 242.0 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 316.5 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 253.2 |
LaF3 (mp-905) | <1 0 1> | <0 1 -1> | 290.8 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 0> | 316.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 316.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 316.5 |
GaP (mp-2490) | <1 1 0> | <1 -1 0> | 221.1 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 -1> | 236.5 |
InSb (mp-20012) | <1 1 0> | <0 1 0> | 316.4 |
NdGaO3 (mp-3196) | <1 0 0> | <1 -1 0> | 221.1 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 -1> | 290.8 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 316.5 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 237.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NbIrS4 (mp-33670) | 0.3451 | 0.103 | 3 |
ZrTiTe4 (mp-8677) | 0.2286 | 0.012 | 3 |
TiNbS4 (mp-34289) | 0.2672 | 0.019 | 3 |
ZrTiSe4 (mp-570062) | 0.3704 | 0.022 | 3 |
BiTeI (mp-22965) | 0.4220 | 0.000 | 3 |
SrLa6OsI12 (mp-567419) | 0.6522 | 0.000 | 4 |
NaLa6OsI12 (mp-569905) | 0.5687 | 0.000 | 4 |
Te6Mo3WS2 (mp-1030333) | 0.7158 | 0.095 | 4 |
Te3MoWS (mp-1029952) | 0.7165 | 0.103 | 4 |
Te6MoW3S2 (mp-1028767) | 0.7133 | 0.108 | 4 |
NbS2 (mp-995122) | 0.2198 | 0.037 | 2 |
VS2 (mp-849054) | 0.2351 | 0.001 | 2 |
TaS2 (mp-755523) | 0.2437 | 0.021 | 2 |
VTe2 (mp-1008626) | 0.2320 | 0.018 | 2 |
VSe2 (mp-684962) | 0.2454 | 0.000 | 2 |
Te4Mo3W(SeS)2 (mp-1030332) | 0.7298 | 0.083 | 5 |
Te4Mo3W(SeS)2 (mp-1027351) | 0.7257 | 0.118 | 5 |
Te2MoWSeS (mp-1027074) | 0.7261 | 0.119 | 5 |
Te4Mo3W(SeS)2 (mp-1027545) | 0.7298 | 0.115 | 5 |
Te2MoWSeS (mp-1027511) | 0.7288 | 0.139 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv Ir Se |
Final Energy/Atom-6.4042 eV |
Corrected Energy-192.1247 eV
-192.1247 eV = -192.1247 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)