Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.173 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.059 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHo2S3 + PbS |
Band Gap2.164 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 298.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 99.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 99.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 298.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 298.3 |
Fe3O4 (mp-19306) | <1 1 0> | <0 0 1> | 99.4 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 298.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 198.9 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 298.3 |
Ga2O3 (mp-886) | <1 1 0> | <0 0 1> | 298.3 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 99.4 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 99.4 |
Si (mp-149) | <1 0 0> | <0 0 1> | 298.3 |
Au (mp-81) | <1 1 0> | <0 0 1> | 99.4 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 298.3 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 298.3 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 298.3 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 298.3 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 0 1> | 198.9 |
MgAl2O4 (mp-3536) | <1 1 0> | <0 0 1> | 99.4 |
GaTe (mp-542812) | <0 0 1> | <0 0 1> | 298.3 |
GaTe (mp-542812) | <1 0 -1> | <1 0 0> | 157.4 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 298.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm3(Bi7Te12)2 (mp-675353) | 0.3462 | 0.132 | 3 |
Tb14(PbSe8)3 (mp-676110) | 0.1888 | 0.043 | 3 |
Dy14(PbS8)3 (mp-675822) | 0.1044 | 0.049 | 3 |
Tb6CdS10 (mp-530870) | 0.2913 | 0.046 | 3 |
Tb6PbSe10 (mp-675130) | 0.2292 | 0.040 | 3 |
TiTlCuTe3 (mp-9344) | 0.7240 | 0.000 | 4 |
Ba20As13 (mp-685008) | 0.3406 | 0.000 | 2 |
Sm39S56 (mp-684860) | 0.3228 | 0.024 | 2 |
Lu2Se3 (mp-673650) | 0.3312 | 0.110 | 2 |
Er2Se3 (mp-32736) | 0.3340 | 0.076 | 2 |
Tm2Se3 (mp-32850) | 0.3276 | 0.087 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ho_3 Pb_d S |
Final Energy/Atom-6.0423 eV |
Corrected Energy-263.6567 eV
-263.6567 eV = -247.7336 eV (uncorrected energy) - 15.9230 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)