Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.377 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.56 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.831 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/m [87] |
Hall-I 4 |
Point Group4/m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 147.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 295.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 221.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 73.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 295.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 147.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 147.6 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 295.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 295.1 |
BN (mp-984) | <1 1 0> | <1 0 1> | 135.8 |
BN (mp-984) | <1 1 1> | <1 0 1> | 135.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 147.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 221.3 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 228.0 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 295.1 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 73.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 221.3 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 73.8 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 73.8 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 1> | 135.8 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 295.1 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 228.0 |
Si (mp-149) | <1 0 0> | <0 0 1> | 147.6 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 73.8 |
C (mp-48) | <1 1 0> | <1 0 1> | 135.8 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 295.1 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 221.3 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 295.1 |
ZnO (mp-2133) | <1 0 1> | <1 1 1> | 177.3 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 295.1 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 295.1 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 147.6 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 73.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 221.3 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 295.1 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 228.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 73.8 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 147.6 |
Au (mp-81) | <1 0 0> | <0 0 1> | 295.1 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 228.0 |
C (mp-48) | <1 1 1> | <1 0 1> | 135.8 |
CaCO3 (mp-3953) | <1 1 0> | <0 0 1> | 147.6 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 295.1 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 114.0 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 161.2 |
CdWO4 (mp-19387) | <1 0 1> | <1 1 1> | 177.3 |
GaTe (mp-542812) | <1 0 1> | <0 0 1> | 295.1 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 295.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
16.77 | 0.00 | 0.01 |
0.00 | 16.78 | 0.01 |
0.01 | 0.01 | 16.67 |
Dielectric Tensor εij (total) |
||
---|---|---|
176.65 | 0.01 | 0.03 |
0.01 | 176.73 | 0.13 |
0.03 | 0.13 | 71.23 |
Polycrystalline dielectric constant
εpoly∞
16.74
|
Polycrystalline dielectric constant
εpoly
141.54
|
Refractive Index n4.09 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tl9SbTe6 (mp-34292) | 0.5188 | 0.000 | 3 |
Tl9BiTe6 (mp-34361) | 0.2685 | 0.000 | 3 |
Tl4Te3Pb (mp-20740) | 0.5428 | 0.000 | 3 |
Tl9SbSe6 (mp-676274) | 0.3261 | 0.000 | 3 |
Tl9SbTe6 (mp-686086) | 0.4883 | 0.004 | 3 |
Tl5Se3 (mp-21657) | 0.4781 | 0.008 | 2 |
Nb5Ga3 (mp-30704) | 0.7367 | 0.253 | 2 |
Tl5Te3 (mp-174) | 0.6055 | 0.011 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d Bi Se |
Final Energy/Atom-3.2598 eV |
Corrected Energy-52.1576 eV
-52.1576 eV = -52.1576 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)