Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.122 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.061 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAg10Te4Br3 + AgBr + Te |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 -1 0> | 205.2 |
AlN (mp-661) | <1 0 1> | <1 -1 0> | 273.6 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 253.7 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 190.3 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 214.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 253.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 317.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 -1 0> | 136.8 |
CeO2 (mp-20194) | <1 0 0> | <1 -1 0> | 273.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 126.9 |
GaAs (mp-2534) | <1 0 0> | <1 -1 0> | 68.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 -1 1> | 257.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 261.0 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 247.3 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 190.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 208.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 208.8 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 317.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 -1 0> | 273.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 -1 0> | 136.8 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 254.3 |
ZnSe (mp-1190) | <1 1 0> | <1 -1 0> | 136.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 254.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 261.0 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 261.0 |
Ag (mp-124) | <1 0 0> | <1 -1 0> | 68.4 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 239.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 126.9 |
LiGaO2 (mp-5854) | <1 0 1> | <1 -1 0> | 136.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 317.8 |
BN (mp-984) | <1 0 0> | <0 1 0> | 190.3 |
Al (mp-134) | <1 0 0> | <1 -1 1> | 257.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 253.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 261.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 190.3 |
LiGaO2 (mp-5854) | <1 1 1> | <1 -1 0> | 273.6 |
TeO2 (mp-2125) | <1 1 0> | <1 -1 0> | 205.2 |
TeO2 (mp-2125) | <1 1 1> | <1 -1 0> | 205.2 |
TiO2 (mp-2657) | <0 0 1> | <1 -1 0> | 273.6 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 317.2 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 253.7 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 208.8 |
Mg (mp-153) | <1 1 1> | <1 1 0> | 214.0 |
LaF3 (mp-905) | <1 1 0> | <0 1 0> | 190.3 |
PbS (mp-21276) | <1 1 0> | <1 -1 0> | 205.2 |
GaP (mp-2490) | <1 0 0> | <1 -1 0> | 273.6 |
GaP (mp-2490) | <1 1 0> | <0 1 0> | 126.9 |
SiC (mp-7631) | <0 0 1> | <1 -1 0> | 205.2 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 0> | 214.0 |
Fe3O4 (mp-19306) | <1 1 0> | <1 -1 0> | 205.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ag8GeTe6 (mp-685969) | 0.6846 | 0.022 | 3 |
La2Fe2S5 (mp-2995) | 0.6823 | 0.132 | 3 |
Ca2CdSb2 (mp-569267) | 0.7160 | 0.000 | 3 |
U2PbSe5 (mp-616821) | 0.7190 | 0.013 | 3 |
Sm3(Sb7Te12)2 (mp-675760) | 0.7229 | 0.124 | 3 |
Te40Rh31 (mp-684876) | 0.6875 | 0.277 | 2 |
MgSi2 (mp-1073495) | 0.6110 | 0.193 | 2 |
MgSi2 (mp-1073604) | 0.7281 | 0.149 | 2 |
Mg5Si9 (mp-1075627) | 0.6573 | 0.194 | 2 |
Mg5Si9 (mp-1075600) | 0.7203 | 0.194 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag Te Br |
Final Energy/Atom-2.8078 eV |
Corrected Energy-44.9255 eV
-44.9255 eV = -44.9255 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)