Final Magnetic Moment13.237 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.425 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.027 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSmGdS3 + GdS |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42d [122] |
HallI 4 2bw |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 285.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 142.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 213.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 284.9 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 213.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 100.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 284.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 284.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 284.9 |
Al (mp-134) | <1 0 0> | <1 1 1> | 247.1 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 213.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 142.5 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 201.5 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 284.9 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 201.5 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 284.9 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 100.7 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 123.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 71.2 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 123.5 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 71.2 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 100.7 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 284.9 |
C (mp-66) | <1 1 0> | <1 1 0> | 201.5 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 284.9 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 284.9 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 71.2 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 100.7 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 71.2 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 284.9 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 213.7 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 100.7 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 142.5 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 100.7 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 284.9 |
C (mp-48) | <1 0 0> | <1 0 0> | 213.7 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 284.9 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 142.5 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 284.9 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 284.9 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 1> | 123.5 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 71.2 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 284.9 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 213.7 |
ZnO (mp-2133) | <1 1 1> | <1 0 0> | 284.9 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 201.5 |
LiAlO2 (mp-3427) | <1 1 1> | <1 0 0> | 284.9 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 284.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca(Pr2Se3)4 (mp-38347) | 0.0717 | 0.016 | 3 |
Nd2SmS4 (mp-38901) | 0.0623 | 0.039 | 3 |
Ca(Ce2Se3)4 (mp-38870) | 0.0619 | 0.004 | 3 |
YbPr11Se16 (mp-531712) | 0.0723 | 0.016 | 3 |
Ce2SmS4 (mp-37045) | 0.0581 | 0.025 | 3 |
Ce4Sb3 (mp-20680) | 0.0437 | 0.000 | 2 |
Tb4Bi3 (mp-570759) | 0.0424 | 0.031 | 2 |
Sm3Te4 (mp-571144) | 0.0429 | 0.000 | 2 |
Sm3Se4 (mp-1344) | 0.0415 | 0.038 | 2 |
Sm3S4 (mp-2038) | 0.0419 | 0.045 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sm_3 Gd S |
Final Energy/Atom-9.1051 eV |
Corrected Energy-131.4951 eV
Uncorrected energy = -127.4711 eV
Composition-based energy adjustment (-0.503 eV/atom x 8.0 atoms) = -4.0240 eV
Corrected energy = -131.4951 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)