Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.680 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaP2H5O8 + NaHSeO4 + Na2SeO4 |
Band Gap3.435 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 -1 1> | 272.0 |
AlN (mp-661) | <0 0 1> | <1 1 -1> | 271.4 |
AlN (mp-661) | <1 0 0> | <0 1 -1> | 297.0 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 266.7 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 210.8 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 256.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 235.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 255.0 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 140.5 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 207.4 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 153.8 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 199.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 153.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 259.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 313.4 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 235.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 255.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 259.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 210.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 140.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 281.1 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 207.4 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 140.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 70.3 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 210.8 |
CdS (mp-672) | <1 0 0> | <0 1 -1> | 222.8 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 230.6 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 156.7 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 70.3 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 259.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 207.4 |
Te2W (mp-22693) | <0 1 0> | <0 1 -1> | 222.8 |
Te2W (mp-22693) | <0 1 1> | <1 1 -1> | 181.0 |
Te2W (mp-22693) | <1 0 0> | <1 1 1> | 307.5 |
Te2W (mp-22693) | <1 1 0> | <0 1 -1> | 222.8 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 210.8 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 140.5 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 70.3 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 235.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 155.6 |
Te2Mo (mp-602) | <1 0 0> | <0 1 -1> | 222.8 |
Te2Mo (mp-602) | <1 0 1> | <0 1 -1> | 222.8 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 266.5 |
BN (mp-984) | <0 0 1> | <1 1 -1> | 181.0 |
BN (mp-984) | <1 0 0> | <1 0 0> | 207.4 |
BN (mp-984) | <1 0 1> | <1 0 0> | 155.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 210.8 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 307.4 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 207.4 |
Al (mp-134) | <1 1 0> | <0 1 1> | 70.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiP3W2O13 (mp-763452) | 0.6882 | 0.048 | 4 |
Na3H(SO4)2 (mp-23780) | 0.6396 | 0.000 | 4 |
Ca2P2H8O11 (mp-554174) | 0.6879 | 0.016 | 4 |
Na3H(SO4)2 (mp-707941) | 0.5775 | 0.001 | 4 |
Na5H7(Se2O9)2 (mp-722267) | 0.4811 | 0.005 | 4 |
NaCoP2HO7 (mp-698706) | 0.5481 | 0.172 | 5 |
LiMnP2HO7 (mp-780113) | 0.6037 | 0.067 | 5 |
NaZnP2HO7 (mp-23799) | 0.5944 | 0.018 | 5 |
NaNiP2HO7 (mp-743636) | 0.5892 | 0.000 | 5 |
K2CdH4(SeO5)2 (mp-697945) | 0.6007 | 0.000 | 5 |
K3Na3TeP6(HO4)6 (mp-707985) | 0.7153 | 0.059 | 6 |
NaCoBP2H2O9 (mp-601388) | 0.6330 | 0.072 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv P H Se O |
Final Energy/Atom-5.3111 eV |
Corrected Energy-165.2587 eV
-165.2587 eV = -154.0221 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)