Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-4.047 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.158 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaHoF4 + HoF3 |
Band Gap5.828 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 329.0 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 122.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 92.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 188.3 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 121.8 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 112.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 168.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 230.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 199.4 |
GaAs (mp-2534) | <1 0 0> | <1 -1 0> | 168.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 193.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 122.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 276.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 214.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 138.1 |
GaN (mp-804) | <1 0 1> | <1 -1 0> | 168.2 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 112.3 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 121.8 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 203.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 187.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 262.1 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 276.2 |
SiO2 (mp-6930) | <0 0 1> | <1 -1 0> | 336.3 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 112.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 226.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 322.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 122.7 |
ZnSe (mp-1190) | <1 0 0> | <1 -1 0> | 168.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 193.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 121.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 -1 1> | 270.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 193.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 284.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 113.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 -1 1> | 225.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 184.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 276.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 113.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 301.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 230.1 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 162.4 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 203.0 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 205.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 150.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 168.8 |
LiF (mp-1138) | <1 1 1> | <1 -1 1> | 225.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 149.8 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 168.8 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 230.1 |
YVO4 (mp-19133) | <0 0 1> | <1 -1 0> | 210.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Bi4O3F7 (mp-753832) | 0.7079 | 0.087 | 3 |
KBi2F7 (mp-675634) | 0.5998 | 0.069 | 3 |
Tb2Mg3Ni2 (mp-570272) | 0.6289 | 0.000 | 3 |
Ba3Y2Cl12 (mp-768972) | 0.6826 | 0.060 | 3 |
Ba3Y2Br12 (mp-768399) | 0.5590 | 0.071 | 3 |
Rb4Pb9 (mp-680463) | 0.6477 | 0.000 | 2 |
MgSi2 (mp-1073613) | 0.6242 | 0.260 | 2 |
Mg4Si3 (mp-1074259) | 0.5834 | 0.155 | 2 |
Mg5Si6 (mp-1075464) | 0.6362 | 0.237 | 2 |
Mg5Si6 (mp-1075363) | 0.5628 | 0.184 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Ho_3 F |
Final Energy/Atom-6.0889 eV |
Corrected Energy-60.8889 eV
-60.8889 eV = -60.8889 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)