Final Magnetic Moment0.014 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.404 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.249 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToClO2 + NbCl5 + NbCl3O |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 -1> | 299.3 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 296.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 -1> | 299.3 |
LaAlO3 (mp-2920) | <1 1 0> | <1 -1 -1> | 246.7 |
LaAlO3 (mp-2920) | <1 1 1> | <1 -1 -1> | 246.7 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 181.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 188.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 197.8 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 164.9 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 343.9 |
CeO2 (mp-20194) | <1 0 0> | <1 -1 1> | 270.2 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 164.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 241.8 |
GaAs (mp-2534) | <1 1 0> | <1 -1 1> | 270.2 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 196.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 226.2 |
GaN (mp-804) | <1 0 1> | <1 -1 0> | 132.7 |
GaN (mp-804) | <1 1 0> | <0 1 -1> | 173.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 188.0 |
GaN (mp-804) | <0 0 1> | <1 -1 1> | 54.0 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 120.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 107.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 219.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 -1> | 277.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 87.7 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 241.6 |
KCl (mp-23193) | <1 0 0> | <0 1 -1> | 242.9 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 230.8 |
ZnSe (mp-1190) | <1 1 0> | <1 -1 1> | 270.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 219.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 -1 1> | 270.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 316.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 343.9 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 1> | 270.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 343.9 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 263.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 241.8 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 362.7 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 241.6 |
CdS (mp-672) | <1 0 1> | <0 1 -1> | 312.3 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 316.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 268.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 -1 1> | 270.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 241.8 |
LiF (mp-1138) | <1 1 0> | <1 -1 0> | 221.1 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 263.8 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 296.8 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 295.5 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 219.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 316.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KPO3 (mp-675976) | 0.5103 | 1.511 | 3 |
Se2NCl5 (mp-29124) | 0.5657 | 0.161 | 3 |
VOF3 (mp-765770) | 0.5261 | 0.021 | 3 |
MnAgO4 (mp-657749) | 0.5270 | 0.898 | 3 |
Hg2TeO3 (mp-29510) | 0.5776 | 0.008 | 3 |
KLi2(HO)3 (mp-23945) | 0.6016 | 0.481 | 4 |
KNa2AlH6 (mp-600151) | 0.5747 | 0.155 | 4 |
SrH2I2O (mp-703295) | 0.6509 | 0.000 | 4 |
TlMo2Cl7O2 (mp-566031) | 0.6328 | 0.021 | 4 |
KH2I3O (mp-696649) | 0.6475 | 0.005 | 4 |
OF3 (mp-974002) | 0.5129 | 0.326 | 2 |
ClO2 (mp-23207) | 0.5819 | 0.000 | 2 |
SeBr (mp-570589) | 0.6533 | 0.006 | 2 |
SCl2 (mp-28128) | 0.5733 | 0.053 | 2 |
BiCl3 (mp-22908) | 0.6338 | 0.000 | 2 |
Rb4NaW2N5O (mp-705510) | 0.7354 | 0.969 | 5 |
NaH4CNO2 (mp-706281) | 0.7053 | 0.160 | 5 |
S (mp-608100) | 0.5408 | 0.440 | 1 |
S (mp-655141) | 0.5517 | 0.357 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv Cl O |
Final Energy/Atom-4.7764 eV |
Corrected Energy-34.8393 eV
-34.8393 eV = -33.4347 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)