material

RbHF2

ID:

mp-677103

DOI:

10.17188/1283261


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.538 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.002 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.16 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
RbHF2
Band Gap
6.675 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Ima2 [46]
Hall
I 2 2a
Point Group
mm2
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
C (mp-48) <0 0 1> <1 0 0> 0.001 221.6
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.001 186.7
LaF3 (mp-905) <1 1 0> <1 1 0> 0.009 186.7
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.009 318.9
InP (mp-20351) <1 0 0> <0 0 1> 0.009 35.4
LiAlO2 (mp-3427) <1 1 1> <0 1 0> 0.011 218.4
Ni (mp-23) <1 0 0> <0 0 1> 0.011 318.9
GaN (mp-804) <1 0 0> <0 1 0> 0.012 218.4
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.013 177.2
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.013 318.9
InSb (mp-20012) <1 0 0> <0 0 1> 0.015 177.2
C (mp-48) <1 0 0> <0 1 0> 0.016 174.7
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.016 318.9
CdTe (mp-406) <1 0 0> <0 0 1> 0.018 177.2
C (mp-66) <1 0 0> <0 1 1> 0.020 281.2
InP (mp-20351) <1 1 0> <0 0 1> 0.020 248.0
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.022 318.9
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.030 311.1
Te2W (mp-22693) <0 0 1> <1 1 1> 0.032 286.4
ZnO (mp-2133) <0 0 1> <0 1 0> 0.032 349.4
GaN (mp-804) <1 1 1> <0 1 1> 0.034 337.5
TiO2 (mp-2657) <1 0 1> <1 1 1> 0.036 286.4
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.037 212.6
BN (mp-984) <0 0 1> <0 1 1> 0.040 281.2
Ga2O3 (mp-886) <0 1 0> <0 1 1> 0.040 281.2
CdS (mp-672) <0 0 1> <1 1 0> 0.042 62.2
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.043 177.2
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.045 283.5
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.045 70.9
AlN (mp-661) <1 1 1> <1 0 0> 0.046 310.3
CdWO4 (mp-19387) <1 1 1> <0 1 0> 0.048 305.7
MgO (mp-1265) <1 1 1> <0 0 1> 0.049 248.0
GaN (mp-804) <1 1 0> <0 0 1> 0.050 318.9
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.051 141.7
PbS (mp-21276) <1 0 0> <0 0 1> 0.052 35.4
Au (mp-81) <1 0 0> <0 0 1> 0.055 35.4
CdWO4 (mp-19387) <1 0 1> <0 1 0> 0.057 43.7
Ag (mp-124) <1 1 0> <0 1 1> 0.059 168.7
YAlO3 (mp-3792) <1 0 1> <0 1 0> 0.059 349.4
Ag (mp-124) <1 1 1> <0 0 1> 0.060 177.2
KTaO3 (mp-3614) <1 1 1> <1 1 0> 0.062 248.9
GaTe (mp-542812) <1 0 -1> <1 1 0> 0.062 311.1
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.063 354.4
Bi2Se3 (mp-541837) <1 0 0> <0 0 1> 0.064 248.0
WS2 (mp-224) <1 0 1> <0 1 1> 0.064 281.2
GaN (mp-804) <0 0 1> <0 1 0> 0.065 349.4
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.066 141.7
TiO2 (mp-2657) <1 0 0> <0 1 1> 0.071 56.2
CdS (mp-672) <1 1 0> <1 1 0> 0.073 248.9
ZnO (mp-2133) <1 0 1> <0 1 0> 0.074 174.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
36 20 12 0 0 0
20 37 12 0 0 0
12 12 40 0 0 0
0 0 0 8 0 0
0 0 0 0 8 0
0 0 0 0 0 17
Compliance Tensor Sij (10-12Pa-1)
40.8 -20.4 -6.1 0 0 0
-20.4 40.6 -6.1 0 0 0
-6.1 -6.1 28.8 0 0 0
0 0 0 132.3 0 0
0 0 0 0 132.6 0
0 0 0 0 0 59.6
Shear Modulus GV
11 GPa
Bulk Modulus KV
22 GPa
Shear Modulus GR
10 GPa
Bulk Modulus KR
22 GPa
Shear Modulus GVRH
10 GPa
Bulk Modulus KVRH
22 GPa
Elastic Anisotropy
0.64
Poisson's Ratio
0.30

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
-0.10769 -0.10506 -0.05766 0.00000 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 -0.04064
0.00000 0.00000 0.00000 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.16112 C/m2
Crystallographic Direction vmax
1.00000
0.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
1.93 0.00 0.00
0.00 1.90 0.00
0.00 0.00 1.95
Dielectric Tensor εij (total)
7.94 0.00 0.00
0.00 5.64 0.00
0.00 0.00 6.61
Polycrystalline dielectric constant εpoly
(electronic contribution)
1.93
Polycrystalline dielectric constant εpoly
(total)
6.73
Refractive Index n
1.39
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
KHF2 (mp-23846) 0.1573 0.000 3
CsSrN9 (mp-29228) 0.5033 0.008 3
Cs2SrN12 (mp-621930) 0.6064 0.009 3
CsHF2 (mp-24668) 0.1972 0.000 3
RbHF2 (mp-29764) 0.1467 0.000 3
KCSN (mp-6511) 0.4560 0.004 4
PbC2(SN)2 (mp-20605) 0.5340 0.139 4
EuC2(SN)2 (mp-22175) 0.5861 0.073 4
SrC2(SN)2 (mp-10927) 0.5707 0.032 4
BaC2(SN)2 (mp-10928) 0.5189 0.016 4
CaN6 (mp-676) 0.4658 0.000 2
CsN3 (mp-510557) 0.2005 0.000 2
RbN3 (mp-743) 0.2206 0.000 2
TlN3 (mp-870) 0.2684 0.041 2
KN3 (mp-827) 0.2376 0.000 2
Cs5Ag4C8IN8 (mp-683972) 0.6829 0.135 5
RbBiC4(SN)4 (mp-647987) 0.7105 0.156 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Rb_sv H F
Final Energy/Atom
-4.3034 eV
Corrected Energy
-36.2756 eV
Uncorrected energy = -34.4276 eV Composition-based energy adjustment (-0.462 eV/atom x 4.0 atoms) = -1.8480 eV Corrected energy = -36.2756 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • Ordering of Disordered Crystal

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)