Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.886 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.108 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAlTlSiO4 + NaAlSiO4 |
Band Gap2.938 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4mm [99] |
HallP 4 2 |
Point Group4mm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 155.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 155.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 155.9 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 155.9 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 155.9 |
Au (mp-81) | <1 0 0> | <1 0 0> | 155.9 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 155.9 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 155.9 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 155.9 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 155.9 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 155.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SiSnO3 (mp-776110) | 0.6698 | 0.026 | 3 |
Mn2Si4O11 (mp-768088) | 0.6817 | 0.090 | 3 |
LiVSi3O8 (mp-767324) | 0.6352 | 0.053 | 4 |
LiSi3BiO8 (mp-766179) | 0.5528 | 0.079 | 4 |
K2Zn2Si8O19 (mp-559127) | 0.6600 | 0.006 | 4 |
LiSi2BO6 (mp-556531) | 0.6331 | 0.000 | 4 |
LiSi3BiO8 (mp-757127) | 0.6235 | 0.095 | 4 |
Na7Al10Si14(AgO16)3 (mp-690987) | 0.5691 | 0.111 | 5 |
Na7Al11Si13(AgO12)4 (mp-686232) | 0.6175 | 0.163 | 5 |
K6Al11Si13Ag5O48 (mp-686585) | 0.3929 | 0.171 | 5 |
Rb9Na2Al11Si13O48 (mp-720212) | 0.5781 | 0.114 | 5 |
Na4Al11Si13Ag7O48 (mp-695373) | 0.5975 | 0.126 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Al Tl_d Si O |
Final Energy/Atom-6.9099 eV |
Corrected Energy-614.1432 eV
-614.1432 eV = -580.4333 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)