Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.349 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.296 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHC2N3 + CS14 + H4NCl + SCl + C |
Band Gap0.095 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <1 -1 1> | 171.5 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 264.0 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 264.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 264.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 132.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 101.5 |
BN (mp-984) | <1 0 0> | <0 1 1> | 153.6 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 209.1 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 209.1 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 209.1 |
C (mp-66) | <1 0 0> | <0 1 1> | 153.6 |
C (mp-66) | <1 1 1> | <1 0 -1> | 132.0 |
LaF3 (mp-905) | <1 0 0> | <1 0 -1> | 264.0 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 203.1 |
PbS (mp-21276) | <1 1 0> | <1 0 -1> | 264.0 |
GaP (mp-2490) | <1 1 0> | <1 -1 1> | 171.5 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 264.0 |
Si (mp-149) | <1 1 0> | <1 -1 1> | 171.5 |
NdGaO3 (mp-3196) | <0 1 0> | <1 -1 1> | 171.5 |
MoSe2 (mp-1634) | <1 0 0> | <0 1 1> | 153.6 |
C (mp-48) | <1 0 0> | <0 1 1> | 153.6 |
CdSe (mp-2691) | <1 1 0> | <1 0 -1> | 264.0 |
WSe2 (mp-1821) | <1 0 0> | <0 1 1> | 153.6 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 -1> | 132.0 |
SiC (mp-8062) | <1 1 0> | <1 -1 -1> | 165.0 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 101.5 |
CdWO4 (mp-19387) | <0 1 0> | <1 1 0> | 158.0 |
CdWO4 (mp-19387) | <0 1 1> | <1 0 1> | 158.3 |
CsI (mp-614603) | <1 1 0> | <1 -1 1> | 171.5 |
GaSb (mp-1156) | <1 1 0> | <1 0 -1> | 264.0 |
CaF2 (mp-2741) | <1 1 0> | <1 -1 1> | 171.5 |
Fe2O3 (mp-24972) | <1 0 0> | <1 0 0> | 209.1 |
ZnTe (mp-2176) | <1 1 0> | <1 0 -1> | 264.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H22C10O3 (mp-707412) | 0.7116 | 0.347 | 3 |
HCO (mp-995234) | 0.6063 | 0.265 | 3 |
Be(N3O7)2 (mp-30141) | 0.6504 | 0.055 | 3 |
H2NO2 (mp-28349) | 0.7341 | 0.207 | 3 |
C4O5F6 (mp-556192) | 0.7056 | 0.131 | 3 |
H4CN2O (mp-720526) | 0.6732 | 0.134 | 4 |
H8C3(NO)4 (mp-708965) | 0.6587 | 0.570 | 4 |
H9C5NO5 (mp-558863) | 0.6755 | 0.268 | 4 |
SrB6(H4O7)2 (mp-721618) | 0.6640 | 0.004 | 4 |
PCN2Cl3 (mp-679969) | 0.6284 | 0.044 | 4 |
ZnH8C4(NO3)2 (mp-655017) | 0.5911 | 0.584 | 5 |
Cr4H67C20(NO)16 (mp-706251) | 0.6168 | 0.275 | 5 |
ZnH8C4(NO3)2 (mp-601243) | 0.5753 | 0.584 | 5 |
P3H22C3N9O11 (mp-720461) | 0.6243 | 0.026 | 5 |
B3H52C16(NO)12 (mp-699412) | 0.6121 | 0.283 | 5 |
NaH18C9I(NO)3 (mp-720100) | 0.6141 | 0.612 | 6 |
AgH9C7S2(OF)4 (mp-555250) | 0.7395 | 0.251 | 6 |
PH10C3N2O4F (mp-558845) | 0.7248 | 0.133 | 6 |
H6C3SN3O2F3 (mp-555728) | 0.7251 | 0.366 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: H C S N Cl |
Final Energy/Atom-5.1397 eV |
Corrected Energy-302.0853 eV
-302.0853 eV = -298.1046 eV (uncorrected energy) - 3.9808 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)