Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.842 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.314 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP321 [150] |
HallP 3 2" |
Point Group32 |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 181.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 174.4 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 290.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 302.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 241.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 60.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 223.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 241.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 130.8 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 87.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 348.8 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 223.6 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 1> | 290.2 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 223.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 302.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 241.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 60.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 60.4 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 223.6 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 130.8 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 302.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 302.2 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 261.6 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 174.4 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 226.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 261.6 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 181.3 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 87.2 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 226.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 305.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 302.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 241.7 |
BN (mp-984) | <1 0 0> | <1 0 0> | 305.2 |
BN (mp-984) | <1 0 1> | <1 0 0> | 261.6 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 218.0 |
LiTaO3 (mp-3666) | <1 0 1> | <1 0 0> | 305.2 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 218.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 181.3 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 302.2 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 348.8 |
BN (mp-984) | <1 1 0> | <1 0 1> | 298.1 |
BN (mp-984) | <1 1 1> | <0 0 1> | 241.7 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 75.5 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 305.2 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 305.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 60.4 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 348.8 |
C (mp-66) | <1 0 0> | <0 0 1> | 302.2 |
C (mp-66) | <1 1 0> | <1 1 1> | 290.2 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 298.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiBeH3 (mp-977298) | 0.7379 | 0.018 | 3 |
LaMoN3 (mp-989631) | 0.7464 | 0.000 | 3 |
Sr5(Ga3O7)2 (mp-1020709) | 0.6854 | 0.012 | 3 |
CaFeAsO5 (mvc-5813) | 0.4971 | 0.249 | 4 |
CaNiAsO5 (mvc-5683) | 0.4771 | 0.051 | 4 |
CaCrAsO5 (mvc-5561) | 0.4809 | 0.193 | 4 |
CaVAsO5 (mvc-5576) | 0.4956 | 0.066 | 4 |
Ca3ZnGe5O14 (mp-1019566) | 0.1986 | 0.023 | 4 |
Ca3TaGa3(SiO7)2 (mp-6853) | 0.3438 | 0.000 | 5 |
Nd3Al3Si3(NO6)2 (mp-695170) | 0.4956 | 0.006 | 5 |
La3Zn3Ge2SbO14 (mp-672262) | 0.2742 | 0.009 | 5 |
Zn3TeAs2Pb3O14 (mp-558298) | 0.5172 | 0.000 | 5 |
Sr3TaGa3(SiO7)2 (mp-16136) | 0.4952 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Ga_d Sn_d O |
Final Energy/Atom-6.9023 eV |
Corrected Energy-168.3699 eV
Uncorrected energy = -158.7519 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Corrected energy = -168.3699 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)