Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.961 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.226 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCO2 + Os + C |
Band Gap2.651 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 260.3 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 260.3 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 260.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 173.6 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 173.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 260.3 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 134.0 |
Te2Mo (mp-602) | <1 0 0> | <1 -1 -1> | 166.5 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 260.3 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 260.3 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 260.3 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 260.3 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 260.3 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 260.3 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 260.3 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 260.3 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 86.8 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 260.3 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 0> | 134.0 |
Au (mp-81) | <1 0 0> | <0 1 -1> | 157.8 |
C (mp-48) | <0 0 1> | <0 0 1> | 173.6 |
ZrO2 (mp-2858) | <0 1 1> | <0 1 -1> | 157.8 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 260.3 |
SiC (mp-8062) | <1 1 0> | <1 -1 1> | 189.1 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 260.3 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 1> | 176.2 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 260.3 |
Cu (mp-30) | <1 1 0> | <1 -1 -1> | 166.5 |
SrTiO3 (mp-4651) | <1 0 0> | <0 0 1> | 86.8 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 260.3 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 260.3 |
Al2O3 (mp-1143) | <1 0 1> | <0 0 1> | 260.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ru(CO)4 (mp-616541) | 0.4765 | 0.270 | 3 |
Ru(CO)4 (mp-655353) | 0.4977 | 0.220 | 3 |
Os(CO)4 (mp-640748) | 0.3109 | 0.214 | 3 |
Ru(CO)4 (mp-652407) | 0.3314 | 0.221 | 3 |
Os6C19O20 (mp-648157) | 0.4504 | 0.225 | 3 |
PtC2(ClO)2 (mp-618423) | 0.5244 | 0.098 | 4 |
Co3C10ClO9 (mp-623047) | 0.5160 | 0.457 | 4 |
Os3C12(IO6)2 (mp-621944) | 0.3548 | 0.170 | 4 |
Fe4Pb(CO)16 (mp-652092) | 0.5259 | 0.707 | 4 |
Os2Pt(CO)9 (mp-650695) | 0.3542 | 0.220 | 4 |
XeF3 (mp-561153) | 0.7397 | 0.000 | 2 |
H2Ru6C18SO20 (mp-720807) | 0.6591 | 0.183 | 5 |
Si2Os3C12(ClO2)6 (mp-648117) | 0.7291 | 0.211 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Os_pv C O |
Final Energy/Atom-8.1964 eV |
Corrected Energy-612.6132 eV
-612.6132 eV = -590.1399 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)