Final Magnetic Moment0.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.454 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom< 0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSb3Pd8 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 206.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 51.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 310.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 206.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 155.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 206.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 310.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 206.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 206.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 206.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 258.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 206.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 206.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 103.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 51.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 206.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 206.7 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 258.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 258.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 206.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 206.7 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 258.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 258.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 206.7 |
C (mp-66) | <1 1 1> | <0 0 1> | 155.0 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 155.0 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 51.7 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 258.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 206.7 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 206.7 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 310.0 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 310.0 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 206.7 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 310.0 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 258.3 |
Au (mp-81) | <1 1 1> | <0 0 1> | 206.7 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 206.7 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 310.0 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 155.0 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 155.0 |
Si (mp-149) | <1 1 0> | <0 0 1> | 206.7 |
Si (mp-149) | <1 1 1> | <0 0 1> | 51.7 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 206.7 |
C (mp-48) | <0 0 1> | <0 0 1> | 206.7 |
C (mp-48) | <1 0 0> | <0 0 1> | 206.7 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 155.0 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 310.0 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 258.3 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 258.3 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 258.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Yb8In3 (mp-680653) | 0.4583 | 0.000 | 2 |
Na8Hg3 (mp-541787) | 0.3198 | 0.000 | 2 |
Ni8P3 (mp-14513) | 0.5005 | 0.002 | 2 |
Mg9Si5 (mp-1074095) | 0.7456 | 0.253 | 2 |
Al3Au8 (mp-16480) | 0.4714 | 0.002 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sb Pd |
Final Energy/Atom-5.3450 eV |
Corrected Energy-235.1798 eV
-235.1798 eV = -235.1798 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)