Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.040 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.331 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCccm [66] |
Hall-C 2 2c |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 265.3 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 132.7 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 132.7 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 265.3 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 132.7 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 132.7 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 132.7 |
CsI (mp-614603) | <1 1 0> | <0 0 1> | 265.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BiPS4 (mp-27133) | 0.6836 | 0.000 | 3 |
NaGaBr4 (mp-28679) | 0.6880 | 0.000 | 3 |
NaAlI4 (mp-29395) | 0.7277 | 0.000 | 3 |
InGaBr4 (mp-541283) | 0.6986 | 0.000 | 3 |
SrNi(PO4)2 (mvc-15098) | 0.6911 | 0.149 | 4 |
K2NaMnO4 (mp-616689) | 0.4851 | 0.000 | 4 |
Ba2CaWN4 (mp-669377) | 0.4894 | 0.004 | 4 |
Na3Bi(PO4)2 (mp-561083) | 0.6480 | 0.000 | 4 |
Na3Ce(PO4)2 (mp-556334) | 0.6858 | 0.000 | 4 |
LiVPHO5 (mp-850399) | 0.7177 | 0.076 | 5 |
Sr6Li2Cr2N8O (mp-565485) | 0.7083 | 0.246 | 5 |
K2CuS(ClO2)2 (mp-560601) | 0.6655 | 0.000 | 5 |
Ba4LaGe3SbSe13 (mp-683936) | 0.6691 | 0.000 | 5 |
BaCaVP2O9 (mvc-16553) | 0.6271 | 0.003 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv As O |
Final Energy/Atom-5.1618 eV |
Corrected Energy-352.8300 eV
-352.8300 eV = -330.3567 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)