Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.225 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 236.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 236.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 236.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 236.3 |
BN (mp-984) | <1 1 1> | <0 0 1> | 236.3 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 236.3 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 236.3 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 236.3 |
C (mp-48) | <1 1 1> | <0 0 1> | 236.3 |
WS2 (mp-224) | <1 0 1> | <0 0 1> | 236.3 |
C (mp-48) | <1 1 0> | <0 0 1> | 236.3 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 236.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb14Si10O17 (mp-680306) | 0.0716 | 0.002 | 3 |
Cs10Si7O9 (mp-581173) | 0.5861 | 0.002 | 3 |
Rb10Si6O17 (mp-556390) | 0.5903 | 0.001 | 3 |
K3W2N5 (mp-1029938) | 0.6032 | 0.000 | 3 |
Rb3W2N5 (mp-1029857) | 0.5498 | 0.000 | 3 |
K13Na2W7N19 (mp-569918) | 0.5713 | 0.006 | 4 |
Pr2Te4MoO14 (mp-566586) | 0.5792 | 0.000 | 4 |
Nd2Te4MoO14 (mp-566059) | 0.5857 | 0.003 | 4 |
K3Al2(PO4)3 (mp-560629) | 0.6340 | 0.000 | 4 |
Cs5Si3AgO9 (mp-554842) | 0.5786 | 0.000 | 4 |
Ca2Cu2Si3(HO3)4 (mp-696360) | 0.7094 | 0.200 | 5 |
LiMnP2HO7 (mp-780584) | 0.6536 | 0.045 | 5 |
K2Cr2AsHO10 (mp-744205) | 0.7143 | 0.000 | 5 |
K2Cr2AsHO10 (mp-744181) | 0.7142 | 0.000 | 5 |
Li2SbSO4F3 (mp-769153) | 0.6452 | 0.069 | 5 |
Na2TeHSO5F3 (mp-696485) | 0.6409 | 0.016 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Si Ge_d O |
Final Energy/Atom-5.5645 eV |
Corrected Energy-959.2985 eV
Uncorrected energy = -912.5825 eV
Composition-based energy adjustment (-0.687 eV/atom x 68.0 atoms) = -46.7160 eV
Corrected energy = -959.2985 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)