Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.153 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToKPb2 + Pb |
Band Gap0.281 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 264.7 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 264.7 |
MoSe2 (mp-1634) | <1 0 1> | <0 0 1> | 264.7 |
ZrO2 (mp-2858) | <0 1 1> | <0 1 0> | 155.0 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 264.7 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 264.7 |
CsI (mp-614603) | <1 1 0> | <0 0 1> | 264.7 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 264.7 |
SrTiO3 (mp-4651) | <1 0 0> | <0 0 1> | 132.3 |
CaF2 (mp-2741) | <1 1 0> | <0 0 1> | 132.3 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 264.7 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 132.3 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 264.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaHo2F7 (mp-676779) | 0.6554 | 0.158 | 3 |
KBi2F7 (mp-675634) | 0.6224 | 0.069 | 3 |
Cr2B2Ir (mp-569911) | 0.6436 | 0.070 | 3 |
Cs5(KPb6)3 (mp-581775) | 0.5891 | 0.006 | 3 |
Tb2Mg3Ni2 (mp-570272) | 0.5938 | 0.000 | 3 |
Rb4Pb9 (mp-680463) | 0.2023 | 0.000 | 2 |
Mg4Si3 (mp-1074388) | 0.5285 | 0.266 | 2 |
Mg7Si4 (mp-1074788) | 0.5397 | 0.169 | 2 |
Mg3Si4 (mp-1075012) | 0.5327 | 0.226 | 2 |
Mg5Si6 (mp-1075464) | 0.5415 | 0.236 | 2 |
Rb (mp-640416) | 0.7401 | 0.057 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Pb_d |
Final Energy/Atom-3.0652 eV |
Corrected Energy-159.3925 eV
-159.3925 eV = -159.3925 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)