Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.305 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.180 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaPb + Ca2Pb + Mn |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mcm [193] |
Hall-P 6c 2 |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 235.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 329.5 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 329.5 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 235.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 329.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 204.9 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 114.1 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 197.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 329.5 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 114.1 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 204.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 263.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 313.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 235.4 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 263.6 |
MoS2 (mp-1434) | <1 0 0> | <1 0 1> | 204.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 313.8 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 313.8 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 78.5 |
TeO2 (mp-2125) | <0 1 1> | <1 1 0> | 228.3 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 313.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 78.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 263.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 313.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 235.4 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 228.3 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 263.6 |
Al (mp-134) | <1 1 0> | <1 0 1> | 204.9 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 235.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 313.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 329.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 197.7 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 313.8 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 78.5 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 263.6 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 329.5 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 78.5 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 1 0> | 228.3 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 131.8 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 156.9 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 156.9 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 1> | 204.9 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 329.5 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 329.5 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 313.8 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 235.4 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 131.8 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 329.5 |
MoSe2 (mp-1634) | <1 1 0> | <1 0 0> | 263.6 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 329.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca5FePb3 (mp-686764) | 0.4930 | 0.336 | 3 |
La5Bi3Br (mp-30212) | 0.4800 | 0.000 | 3 |
La5Pb3I (mp-31288) | 0.4834 | 0.000 | 3 |
La5Sb3Br (mp-29684) | 0.4539 | 0.000 | 3 |
La5Sn3I (mp-569986) | 0.4583 | 0.000 | 3 |
Gd3Ti2MnSi3 (mp-569019) | 0.5070 | 0.407 | 4 |
U5Ge4 (mp-505302) | 0.5662 | 0.047 | 2 |
Nb5Ga4 (mp-18032) | 0.5350 | 0.008 | 2 |
Th5Sn4 (mp-30874) | 0.5758 | 0.000 | 2 |
Ti5Ga4 (mp-30675) | 0.5095 | 0.010 | 2 |
Zr5Al4 (mp-570774) | 0.4969 | 0.047 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Mn_pv Pb_d |
Final Energy/Atom-3.6717 eV |
Corrected Energy-66.0908 eV
Uncorrected energy = -66.0908 eV
Corrected energy = -66.0908 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)