material

NaF

ID:

mp-682

DOI:

10.17188/1282196


Tags: Sodium fluoride (1/1) Villiaumite Sodium fluoride

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.939 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.69 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
6.095 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 29128 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdSe (mp-2691) <1 1 1> <1 1 1> 0.000 267.4
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.000 114.6
WS2 (mp-224) <0 0 1> <1 1 1> 0.000 114.6
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.000 152.8
GaAs (mp-2534) <1 1 0> <1 1 0> 0.000 93.6
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.000 22.1
BN (mp-984) <0 0 1> <1 1 1> 0.001 38.2
GaSb (mp-1156) <1 1 1> <1 1 1> 0.001 267.4
InSb (mp-20012) <1 1 0> <1 1 0> 0.001 62.4
InSb (mp-20012) <1 0 0> <1 0 0> 0.001 44.1
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.002 132.3
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.002 93.6
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.003 38.2
CdTe (mp-406) <1 1 0> <1 1 0> 0.003 62.4
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.003 38.2
CdTe (mp-406) <1 0 0> <1 0 0> 0.003 44.1
Ge (mp-32) <1 1 0> <1 1 0> 0.003 93.6
MgO (mp-1265) <1 1 0> <1 1 0> 0.004 280.7
Mg (mp-153) <0 0 1> <1 1 1> 0.004 114.6
Ni (mp-23) <1 0 0> <1 0 0> 0.005 110.3
PbSe (mp-2201) <1 1 1> <1 1 1> 0.005 267.4
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.005 110.3
InP (mp-20351) <1 0 0> <1 0 0> 0.007 176.4
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.007 198.5
GdScO3 (mp-5690) <0 0 1> <1 1 1> 0.011 191.0
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.014 110.3
LiF (mp-1138) <1 1 1> <1 1 1> 0.015 114.6
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.015 280.7
LiF (mp-1138) <1 1 0> <1 1 0> 0.015 93.6
GaSe (mp-1943) <0 0 1> <1 1 1> 0.018 38.2
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.018 267.4
MgAl2O4 (mp-3536) <1 1 1> <1 1 1> 0.019 114.6
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.019 93.6
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.020 249.5
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.021 311.9
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.022 249.5
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.022 124.8
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.022 152.8
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.022 187.1
InAs (mp-20305) <1 1 1> <1 1 1> 0.023 267.4
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.030 198.5
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.037 152.8
GaAs (mp-2534) <1 0 0> <1 1 1> 0.039 267.4
TbScO3 (mp-31119) <0 0 1> <1 1 1> 0.039 191.0
AlN (mp-661) <1 0 1> <1 1 1> 0.040 267.4
Al (mp-134) <1 1 1> <1 1 1> 0.043 114.6
Al (mp-134) <1 1 0> <1 1 0> 0.044 93.6
C (mp-66) <1 1 1> <1 1 1> 0.044 152.8
Au (mp-81) <1 0 0> <1 0 0> 0.046 88.2
TeO2 (mp-2125) <0 0 1> <1 1 1> 0.046 191.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
95 24 24 0 0 0
24 95 24 0 0 0
24 24 95 0 0 0
0 0 0 27 0 0
0 0 0 0 27 0
0 0 0 0 0 27
Compliance Tensor Sij (10-12Pa-1)
11.7 -2.4 -2.4 0 0 0
-2.4 11.7 -2.4 0 0 0
-2.4 -2.4 11.7 0 0 0
0 0 0 37.2 0 0
0 0 0 0 37.2 0
0 0 0 0 0 37.2
Shear Modulus GV
30 GPa
Bulk Modulus KV
48 GPa
Shear Modulus GR
30 GPa
Bulk Modulus KR
48 GPa
Shear Modulus GVRH
30 GPa
Bulk Modulus KVRH
48 GPa
Elastic Anisotropy
0.09
Poisson's Ratio
0.24

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
1.87 -0.00 0.00
-0.00 1.87 0.00
0.00 0.00 1.87
Dielectric Tensor εij (total)
5.46 -0.00 0.00
-0.00 5.46 0.00
0.00 0.00 5.46
Polycrystalline dielectric constant εpoly
(electronic contribution)
1.87
Polycrystalline dielectric constant εpoly
(total)
5.46
Refractive Index n
1.37
Potentially ferroelectric?
Unknown

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -4.325 13.029 2.517 6.692
pack_evans_james -4.325 13.030 0.279 3.565
vinet -4.326 13.019 2.565 5.486
tait -4.326 13.019 0.282 5.725
birch_euler -4.326 13.027 0.316 0.581
pourier_tarantola -4.326 13.015 0.049 2.652
birch_lagrange -4.328 13.016 0.183 6.322
murnaghan -4.325 13.046 0.272 3.404
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr4SO3 (mp-1079788) 0.0000 0.200 3
BaSr3O4 (mp-984729) 0.0000 0.044 3
ScH4Pd3 (mp-981386) 0.0000 0.114 3
Sr3CdO4 (mp-981103) 0.0000 0.019 3
SrCa3O4 (mp-978844) 0.0000 0.040 3
TmBi (mp-23234) 0.0000 0.000 2
LaSb (mp-1065) 0.0000 0.000 2
NpP (mp-10108) 0.0000 0.000 2
NpS (mp-10109) 0.0000 0.000 2
TbBi (mp-22921) 0.0000 0.000 2
Sc (mp-1008681) 0.0000 0.719 1
Ca (mp-10683) 0.0000 0.400 1
C (mp-998866) 0.0000 2.755 1
Sb (mp-133) 0.0000 0.051 1
Na (mp-1093989) 0.0000 1.084 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
700 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Na_pv F
Final Energy/Atom
-4.3245 eV
Corrected Energy
-9.1110 eV
Uncorrected energy = -8.6490 eV Composition-based energy adjustment (-0.462 eV/atom x 1.0 atoms) = -0.4620 eV Corrected energy = -9.1110 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 262837
  • 29128
  • 41410
  • 44276
  • 41438
  • 53840
  • 52238
  • 53821
  • 43611
  • 262838
Submitted by
User remarks:
  • Sodium fluoride (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)