Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.751 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.889 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPca21 [29] |
HallP 2c 2ac |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <1 1 1> | <0 0 1> | 257.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 257.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 128.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 257.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 128.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 128.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 128.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 128.9 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 128.9 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 128.9 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 257.9 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 128.9 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 128.9 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 128.9 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 128.9 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 128.9 |
NdGaO3 (mp-3196) | <1 0 0> | <0 1 0> | 177.4 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 257.9 |
Si (mp-149) | <1 1 0> | <0 0 1> | 128.9 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 128.9 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 257.9 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 257.9 |
CsI (mp-614603) | <1 1 0> | <0 1 0> | 177.4 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 257.9 |
SrTiO3 (mp-4651) | <1 0 0> | <0 0 1> | 128.9 |
CaF2 (mp-2741) | <1 1 0> | <0 0 1> | 128.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sb3(BrF8)2 (mp-27318) | 0.4984 | 0.000 | 3 |
SrAlH5 (mp-568450) | 0.5372 | 0.000 | 3 |
BaMnF5 (mp-559999) | 0.5461 | 0.129 | 3 |
BaGaF5 (mp-541629) | 0.5332 | 0.000 | 3 |
CsSb2F11 (mp-556061) | 0.4269 | 0.000 | 3 |
Sb2SeI2F11 (mp-558073) | 0.5701 | 0.000 | 4 |
Sb2ClO2F11 (mp-558692) | 0.6607 | 0.000 | 4 |
Sb2SNF11 (mp-560450) | 0.5271 | 0.067 | 4 |
ReTe5O6F25 (mp-649177) | 0.6482 | 0.026 | 4 |
BaTiOF4 (mp-16915) | 0.6485 | 0.000 | 4 |
CrF5 (mp-639662) | 0.5505 | 0.000 | 2 |
Sb7F29 (mp-29369) | 0.5418 | 0.000 | 2 |
VF5 (mp-558797) | 0.5193 | 0.000 | 2 |
VF5 (mp-765273) | 0.5287 | 0.007 | 2 |
VF5 (mp-765241) | 0.4975 | 0.005 | 2 |
HgSb4C2(OF11)2 (mp-556903) | 0.5428 | 0.080 | 5 |
Sb4OsC6(O3F11)2 (mp-558754) | 0.6651 | 0.084 | 5 |
Sb2OsC4(OF3)4 (mp-559010) | 0.6481 | 0.057 | 5 |
Sb4RuC6(O3F11)2 (mp-555952) | 0.6655 | 0.092 | 5 |
FeSb4C6(O3F11)2 (mp-19590) | 0.6697 | 0.242 | 5 |
Sb4IrC5ClO5F22 (mp-555612) | 0.6374 | 0.108 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Sb F |
Final Energy/Atom-4.5511 eV |
Corrected Energy-787.3118 eV
Uncorrected energy = -728.1758 eV
Composition-based energy adjustment (-0.462 eV/atom x 128.0 atoms) = -59.1360 eV
Corrected energy = -787.3118 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)