Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-2.766 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.365 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTa2O5 + Ta |
Band Gap0.766 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/a [88] |
HallI 4bw 1bw |
Point Group4/m |
Crystal Systemtetragonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 274.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 183.3 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 259.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 259.2 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 274.9 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 274.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 274.9 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 274.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 274.9 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 274.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 274.9 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 274.9 |
BN (mp-984) | <1 0 0> | <1 0 0> | 274.9 |
BN (mp-984) | <1 1 0> | <1 0 0> | 274.9 |
BN (mp-984) | <1 1 1> | <1 0 0> | 274.9 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 0> | 91.6 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 0> | 91.6 |
CdWO4 (mp-19387) | <1 0 1> | <1 1 0> | 129.6 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 183.3 |
ZnO (mp-2133) | <1 0 1> | <1 1 0> | 259.2 |
GaSb (mp-1156) | <1 1 1> | <1 0 0> | 274.9 |
SrTiO3 (mp-4651) | <1 1 1> | <1 0 0> | 274.9 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 129.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 274.9 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 274.9 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 183.3 |
ZnTe (mp-2176) | <1 1 1> | <1 0 0> | 274.9 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 183.3 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 259.2 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 183.3 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 259.2 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 259.2 |
PbSe (mp-2201) | <1 1 1> | <1 0 0> | 274.9 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 259.2 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 274.9 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 91.6 |
Au (mp-81) | <1 0 0> | <1 0 0> | 274.9 |
Au (mp-81) | <1 1 0> | <1 0 0> | 274.9 |
CdSe (mp-2691) | <1 1 1> | <1 0 0> | 274.9 |
C (mp-48) | <0 0 1> | <1 0 0> | 274.9 |
C (mp-48) | <1 0 1> | <1 1 0> | 259.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnBiMoO5 (mvc-7861) | 0.7499 | 0.127 | 4 |
SmCuTeS (mp-561248) | 0.7216 | 0.000 | 4 |
LaCuTeS (mp-10288) | 0.7279 | 0.000 | 4 |
Mo3O7 (mvc-9246) | 0.7158 | 0.220 | 2 |
Cr3O7 (mvc-9236) | 0.7098 | 0.152 | 2 |
TaSe2 (mp-542621) | 0.6056 | 0.614 | 2 |
Bi2O3 (mp-556549) | 0.6161 | 0.024 | 2 |
Na3P11 (mp-473) | 0.7035 | 0.000 | 2 |
TiZnO2 (mvc-4616) | 0.6174 | 0.425 | 3 |
Li3SbS3 (mp-775804) | 0.5900 | 0.055 | 3 |
Li3BiS4 (mp-766422) | 0.6366 | 0.065 | 3 |
LiFeF3 (mp-777489) | 0.6227 | 0.090 | 3 |
SbOF (mp-756654) | 0.6131 | 0.083 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points8 |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv O |
Final Energy/Atom-9.5398 eV |
Corrected Energy-480.3831 eV
-480.3831 eV = -457.9098 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)