Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.535 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.038 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiPO3 + LiSb(PO3)4 |
Band Gap3.969 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 339.5 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 145.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 339.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 291.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 194.0 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 242.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 231.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 154.4 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 291.0 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 231.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 231.7 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 182.4 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 145.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 154.4 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 231.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 231.7 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 134.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 145.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 339.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 339.5 |
BN (mp-984) | <1 0 0> | <0 1 0> | 97.0 |
BN (mp-984) | <1 1 1> | <0 1 1> | 273.6 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 127.3 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 339.5 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 231.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 145.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 231.7 |
TeO2 (mp-2125) | <0 1 0> | <0 1 1> | 273.6 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 145.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 308.9 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 77.2 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 242.5 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 339.5 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 154.4 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 1> | 273.6 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 242.5 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 242.5 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 145.5 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 154.4 |
GaP (mp-2490) | <1 1 0> | <0 1 0> | 291.0 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 154.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 308.9 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 154.4 |
NdGaO3 (mp-3196) | <0 1 0> | <0 1 0> | 291.0 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 154.4 |
NdGaO3 (mp-3196) | <1 0 0> | <0 1 0> | 291.0 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 154.4 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 308.9 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 231.7 |
SiC (mp-11714) | <1 1 0> | <0 1 1> | 273.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V5(P3O11)2 (mp-767351) | 0.4185 | 0.020 | 3 |
Si2TeO7 (mvc-4099) | 0.4358 | 0.298 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.4347 | 0.098 | 3 |
Mn5(P3O11)2 (mp-705036) | 0.4563 | 0.065 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.3911 | 0.366 | 3 |
Li2V(PO3)5 (mp-705334) | 0.3838 | 0.046 | 4 |
Li2Cr(PO3)5 (mp-704942) | 0.3713 | 0.088 | 4 |
Li2P5WO15 (mp-763414) | 0.3921 | 0.084 | 4 |
Li2Mo(PO3)5 (mp-540310) | 0.2004 | 0.062 | 4 |
Li2Sn(PO3)5 (mp-757947) | 0.3185 | 0.066 | 4 |
Cr19O48 (mp-850874) | 0.6522 | 0.167 | 2 |
Cr5O12 (mp-19575) | 0.6455 | 0.142 | 2 |
LiVCr(P2O7)2 (mp-767629) | 0.4573 | 0.004 | 5 |
LiMnV(P2O7)2 (mp-764454) | 0.4572 | 0.007 | 5 |
LiVCr(P2O7)2 (mp-767608) | 0.4875 | 0.003 | 5 |
LiVFe(P2O7)2 (mp-767272) | 0.4981 | 0.001 | 5 |
LiVFe(P2O7)2 (mp-765110) | 0.4672 | 0.001 | 5 |
InBP2H5NO9 (mp-752709) | 0.6413 | 0.000 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.4777 | 0.003 | 6 |
VBP2H5NO9 (mp-25798) | 0.6771 | 0.000 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5320 | 0.041 | 6 |
Ca2MnAl2Si3HO13 (mp-745107) | 0.6774 | 0.075 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5373 | 0.068 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sb P O |
Final Energy/Atom-6.8263 eV |
Corrected Energy-334.6194 eV
Uncorrected energy = -314.0094 eV
Composition-based energy adjustment (-0.687 eV/atom x 30.0 atoms) = -20.6100 eV
Corrected energy = -334.6194 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)